Thermal Properties Metric English Comments
Melting Point 114 °C
237 °F
Internal method
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability..
Melting Point 114 °C
237 °F
Internal method
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit..
Melting Point 114 °C
237 °F
Internal method
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a ..
Melting Point 114 °C
237 °F
Internal method
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit..
Melting Point 114 °C
237 °F
Internal method
Polimeri Europa Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FH 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 20 is characterized by a good balance between processability and mechanical properties.Films manufac..
Melting Point 114 °C
237 °F
Internal method
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m..
Melting Point 114 °C
237 °F
Internal method
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion
Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab..
Melting Point 114 °C
237 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin  (discontinued **)
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
Melting Point 114 °C
238 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil LD 117.03 Blown Overwrap Film Resin  (discontinued **)
LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma..
Melting Point 114 °C
238 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil LD 117.08 Blown Overwrap Film Resin  (discontinued **)
LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma..
Melting Point 114 °C
237 °F
LyondellBasell Lupolen® 3010 K LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 114 °C
237 °F
LyondellBasell Lupolen® 3020 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 114 °C
237 °F
LyondellBasell Lupolen® 3020 K LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 114 °C
237 °F
LyondellBasell Lupolen® 3026 F LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 114 °C
237 °F
LyondellBasell Lupolen® 3032 D LDPE
Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 114 °C
237 °F
LyondellBasell Lupolen® 3040 D LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 114 °C
237 °F
LyondellBasell Lupolen® 3220 K LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 114 °C
237 °F
ISO 11357-3
Total FE 8000 LDPE blown film
Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired form..
Melting Point 114 °C
237 °F
ISO 11357-3
Total FE 8004 LDPE blown film
Radical polyethylene made by high pressure autoclave process. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former F..
Melting Point 114 °C
237 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Exceed™ 4518PA Premium Cast Film Resin
Exceed 4518PA resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 4518PA resin have outstanding tensile properties and impact and puncture toughness..
Melting Point 114 °C
237 °F
Freezing Point; ASTM D3418
DuPont™ Bynel® 4033 Anhydride Modified HDPE
BYNEL® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process..
Melting Point 114 °C
237 °F
ASTM D3418, ISO 3146
DuPont™ Fusabond® E528 Polymer Modifier
DuPont™ Fusabond® E528 is a anhydride modified polyethylene. Used as a polymer modifier
Melting Point 114 °C
237 °F
Dow Method (DSC)
Dow FLEXOMER™ DFDA-1095 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDA-1095 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization ..
Melting Point 114 °C
237 °F
Dow Method (DSC)
Dow FLEXOMER™ DFDB-1088 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDB-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to..
Melting Point 114 - 172 °C
237 - 342 °F
Dow Method (DSC)
Dow Saran® 506 Polymer
Saran™ 506 Polymer is designed as an ignition resistant adhesive bonding agent. Saran™ 506 is a vinylidene chloride copolymer supplied as a white, micronized powder. It is unaffected by humidity..
Melting Point 114 °C
237 °F
Dow Method (DSC)
Dow FLEXOMER™ DFDA-1098 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDA-1098 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization ..
Melting Point 114 °C
237 °F
Recrystallizing temperature; ISO 3146
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Melting Point 114 °C
237 °F
Recrystallizing temperature; ISO 3146
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Melting Point 114 - 127 °C
237 - 260 °F
Average value: 119 °C Grade Count:22
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is ..
Melting Point 114 °C
237 °F
ISO 11357-3
Total Lacqtene® 1025 FH 24 LDPE blown film  (discontinued **)
Radical polyethylene made by high pressure tubular process. Slip and antiblock formulated grade for good transparent thin films. Advised temperature profile : 150 to 190°C.Information provided prov..
Copyright © lookpolymers.com All Rights Reserved