| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 125 °C | 257 °F | Internal method |
|
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene
Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h..
|
|||
| Melting Point | 125 °C | 257 °F | Internal method |
|
Polimeri Europa Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FG 106 are characterized by ..
|
|||
| Melting Point | 125 - 130 °C | 257 - 266 °F | |
|
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
|
|||
| Melting Point | 125 - 135 °C | 257 - 275 °F | ASTM D3418 |
|
NatureWorks® Ingeo™ 6302D Fiber Grade PLA
NatureWorks PLA polymer 6302D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6302D is designed for extrusion into mech..
|
|||
| Melting Point | 125 °C | 257 °F | ASTM D3418 |
|
ExxonMobil LLP8455.24 Rotational Molding Resin
(discontinued **)
LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di..
|
|||
| Melting Point | 125 °C | 257 °F | Exxon Method |
|
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st..
|
|||
| Melting Point | 125 °C | 257 °F | Exxon Method |
|
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert..
|
|||
| Melting Point | 125 °C | 257 °F | |
|
Indium Corp. Indalloy 13 Indium Solder Alloy
Information Provided by Indium Corporation
|
|||
| Melting Point | 125 - 129 °C | 257 - 264 °F | Sheath Melt Point; LCL-PR29 |
|
Intercontinental Polymers 1150 Bicomponent HDPE/PET Fiber Type - 3 Denier X 1.5 Inches
50/50 HDPE Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdeni..
|
|||
| Melting Point | 125 - 129 °C | 257 - 264 °F | Sheath Melt Point; LCL-PR29 |
|
Intercontinental Polymers 1171 Bicomponent HDPE/PET Fiber Type - Denier 1.8 X 1.5 Inches
50/50 HDPE Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdeni..
|
|||
| Melting Point | 125 °C | 257 °F | DSC |
|
Lushan DE-1 Polyethylene Sintered Powder
PE sintered powder Lushan DE-1 is combined with more than 10 years practice and experience on the area of oil & gas pipeline anti-corrosion. PE sintered powder Lushan DE-1 is used on anti-corrosion ..
|
|||
| Melting Point | 125 °C | 257 °F | ASTM D2117 |
|
Lushan EP253H Adhesive Resin for Aluminum Plastic Composite Pipe
Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides i..
|
|||
| Melting Point | 125 - 135 °C | 257 - 275 °F | |
|
LG Chemical LUTENE XL8080TR PE Compound
Description: LUTENE XL8080TR has excellent electrical properties for medium and high voltage power cable insulation and especially it shows improved water tree resistance and has thermal aging prope..
|
|||
| Melting Point | 125 - 145 °C | 257 - 293 °F | |
|
Struktol MAGNESIUM STEARATE
High purity stearate with low soluble salt level that reduces discoloration during processing.STRUKTOL® Magnesium Stearate is used by the rubber and plastic industries as an effective elastomer p..
|
|||
| Melting Point | 125 °C | 257 °F | ASTM D2117 |
|
SCG Chemicals EL-Leneâ„¢ M3204 Butene (C4) Rotational Molding Resin
Natural base resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-surf..
|
|||
| Melting Point | 125 °C | 257 °F | ASTM D2117 |
|
SCG Chemicals EL-Leneâ„¢ M40 Butene (C4) Rotational Molding Resin
Color compound resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-su..
|
|||
| Melting Point | 125 °C | 257 °F | No Flow Temp |
|
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Melting Point | 125 °C | 257 °F | ASTM D3418 |
|
Teknor Apex Terraloy™ MB 10000A Thermoplastic Starch + LLDPE
Notes: Terraloy™ MB-10000A is a Thermoplastic Starch/LLDPE masterbatch that contains up to 50% of TPS renewable content. Melt Index for LLDPE for the masterbatch is 0.9. This compound is for brown..
|
|||
| Melting Point | 125 °C | 257 °F | Melting point via DSC/ASTM D3418 |
|
DuPont Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..
|
|||
| Melting Point | 125 °C | 257 °F | Kofler |
|
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio..
|
|||
| Melting Point | 125 °C | 257 °F | ASTM D3418, ISO 3146 |
|
DuPont™ Bynel® 41E755 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
|
|||
| Melting Point | 125 °C | 257 °F | Peak Melting Temperature; ExxonMobil Method |
|
ExxonMobil LL 3201.36 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
|
|||
| Melting Point | 125 °C | 257 °F | ASTM D3418 |
|
ExxonMobil LL 8360.29 Rotational Molding Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..
|
|||
| Melting Point | 125 °C | 257 °F | Dow Method (DSC) |
|
Dow DOWLEX™ 2036G Linear Low Density Polyethylene
Improved thermal stability for high stiffness film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow
|
|||
| Melting Point | 125 °C | 257 °F | Dow Method (DSC) |
|
Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE)
ASPUN™ 6811A Fiber Grade Resin: Suggested Optimum Process: Spun Bond Typical Application: Non-woven FabricsInformation provided by Dow
|
|||
| Melting Point | 125 °C | 257 °F | DSC |
|
Arkema Group OREVAC® 18334 Grafted Maleic Anhydride Polyethylene
OREVAC 18334 is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier bottle. OREVAC 18334 is mainly used in multi-layer bottle and tank to have good adhesio..
|
|||
| Melting Point | 125 °C | 257 °F | ASTM-D3418 |
|
Braskem RA34U3 LLDPE Rotomolding Polyethylene
The resin RA34U3 is a linear low-density polyethylene, 1-butene based, with a good balance of processability, environmental stress cracking resistance, and impact strength. It contains long term UV6..
|
|||
| Melting Point | 125 °C | 257 °F | DSC; ASTM D3418 |
|
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **)
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
|
|||