| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
|
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
|
Murtfeldt Material ”S”® 1000 Green Polyethylene
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
|
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial
Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
|
Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive
Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This m..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
|
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction
This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
|
Murtfeldt Original Material ”S”® plus + TLS Polyethylene
Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i..
|
|||
| Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
|
Okulen® 1000 - REG PE Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
|
Okulen® 1000 PE-UHMW, Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
|
Okulen® 1000 PE-UHMW, Natural
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
|
Okulen® 1000 PE-UHMW, UV - stabilized
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
|
Okulen® 500 - REG PE Colored
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
|
Okulen® 500 - REG PE Multicoloured coarse
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
|
Okulen® 500 PE-HMW, AST
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
|
Okulen® 500 PE-HMW, Coloured
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
|
Okulen® 500 PE-HMW, UV - stabilized
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Melting Point | 125 - 135 °C | 257 - 275 °F | ASTM D3418 |
|
NatureWorks® Ingeo™ 6060D Fiber Grade PLA
NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mech..
|
|||
| Melting Point | 125 - 135 °C | 257 - 275 °F | ASTM D3418 |
|
NatureWorks® Ingeo™ 6302D Fiber Grade PLA
NatureWorks PLA polymer 6302D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6302D is designed for extrusion into mech..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
|
Quadrant EPP Cestilene™ HD 1000 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
|
Quadrant EPP Cestilene™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
|
Quadrant EPP Cestilene™ HD 500 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
|
|||
| Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
|
Okulen® 1000 - REG PE Multicoloured fine
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
|
|||
| Melting Point | 126 - 135 °C | 258 - 275 °F | Average value: 130 °C Grade Count:32 |
|
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
|
|||
| Melting Point | 100 - 135 °C | 212 - 275 °F | |
|
M Chemical GUARD DOGâ„¢ UV944 HALS Light Stabilizer
GUARD DOGâ„¢ UV944 hindered amine light stabilizer is a highly effective radical scavenger that protects polymers against degradation caused by exposure to UV radiation. It is an oligomeric HALS..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | Crystalline melting range |
|
Mikro-Technik Mikrolen UHMW-PE
Properties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at temperatures of -26..
|
|||
| Melting Point | 120 - 135 °C | 248 - 275 °F | |
|
DayGlo ZQ Pigments ZQ-12 Neon Red
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
|
|||
| Melting Point | 120 - 135 °C | 248 - 275 °F | |
|
DayGlo ZQ Pigments ZQ-15 Blaze Orange
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
|
|||
| Melting Point | 120 - 135 °C | 248 - 275 °F | |
|
DayGlo ZQ Pigments ZQ-17 Saturn Yellow
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | DIN 53 736 |
|
Hippe PE 500 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
|
|||
| Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
|
Okulen® 500 PE-HMW, Natural
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Melting Point | 124 - 135 °C | 255 - 275 °F | Average value: 129 °C Grade Count:19 |
|
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..
|
|||