| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 138 - 148 °C | 280 - 298 °F | MQSA 111 |
|
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer
(discontinued **)
PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech..
|
|||
| Melting Point | 138 - 148 °C | 280 - 298 °F | |
|
Fine Organics FINAWAX C Lubricant Additive
Applications: Antiblock agent for soft PVC films/sheets, strong release agent for rigid PVC calendered sheets, dispersant for FRLS PVC compounds.Information provided by Fine Organics
|
|||
| Melting Point | 142 - 148 °C | 288 - 298 °F | DSC; ISO 3146 |
|
Borealis BorPure™ RD226CF Polypropylene Random Copolymer
BorPure™ RD226CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD226CF is recommended for food packaging..
|
|||
| Melting Point | 142 - 148 °C | 288 - 298 °F | DSC; ISO 3146 |
|
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer
BorPure™ RD266CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD266CF is recommended for
food packaging..
|
|||
| Melting Point | 142 - 148 °C | 288 - 298 °F | DSC; ISO 3146 |
|
Borealis BorPURE™ RE216CF Polypropylene Random Copolymer
BorPure™ RE216CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: BorPure™ RE216CF is recommended for Lamination films, Me..
|
|||