| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 148 - 155 °C | 298 - 311 °F | |
| Pau Tai Calcium stearate, Monomer Stabilizer Non sulfide staining and non-toxic. Excellent internal lubricity and good gelation property.Applications: Hard products, non-toxic adhesive plaster and rubber mold release |
|||
| Melting Point | 80.0 - 155 °C | 176 - 311 °F | Average value: 120 °C Grade Count:6 |
| Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
| Melting Point | 122 - 155 °C | 252 - 311 °F | 0.025" extruded film, |
| Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti.. |
|||
| Melting Point | 130 - 155 °C | 266 - 311 °F | Huntsman/TMA |
| Huntsman IROGRAN® A 75 P 4665N TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
| Melting Point | 145 - 155 °C | 293 - 311 °F | Huntsman/TMA |
| Huntsman IROGRAN® A 80 P 5039 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
| Melting Point | 110 - 155 °C | 230 - 311 °F | ISO 3146 |
| Borealis Steripeel™ WD165CF PO Compound for Sterilizable Peelable Film Applications Steripeel WD165CF is a non-formulated film resin, specially developed for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WD165CF is suitable for various peelable.. |
|||
| Melting Point | 110 - 155 °C | 230 - 311 °F | ISO 3146 |
| Borealis Steripeel™ WD170CF PO Compound for Sterilizable Peelable Film Applications Steripeel WD170CF is a non-formulated film resin, specially developed for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WD170CF is suitable for various peelable.. |
|||
| Melting Point | 135 - 155 °C | 275 - 311 °F | ISO 3146 |
| Borealis Steripeel™ WE150CF PO Compound for Sterilizable Peelable Film Applications Steripeel WE150CF is a slip and antiblock agent formulated film resin. It is suitable for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WE150CF is suitable for.. |
|||
| Melting Point | 145 - 155 °C | 293 - 311 °F | DSC |
| EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
| Melting Point | 145 - 155 °C | 293 - 311 °F | DSC |
| EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
| Melting Point | 140 - 155 °C | 284 - 311 °F | DSC |
| BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
| Melting Point | 151 - 155 °C | 304 - 311 °F | |
| Arkema Group KYNAR® LBG2 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc. |
|||
| Melting Point | 137 - 155 °C | 279 - 311 °F | Average value: 146 °C Grade Count:11 |
| Overview of materials for Ethyl Cellulose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ethyl Cellulose, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
| Melting Point | 140 - 155 °C | 284 - 311 °F | DSC |
| BASF Ecovio® C2203 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||