| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 160 °C | 320 °F | |
|
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
|
|||
| Melting Point | 160 °C | 320 °F | |
|
Plastcom SLOVALEN PH 49 GF 40 PP, 40% glass fibre
PP homopolymer for injection moulding, chemically strengthened with 40% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go..
|
|||
| Melting Point | 160 °C | 320 °F | |
|
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant
FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin..
|
|||
| Melting Point | 160 °C | 320 °F | |
|
Plastcom SLOVALEN PH 99 GB 20 PP, 20% glass beads, mod. of mech. prop.
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
|
|||
| Melting Point | 160 - 170 °C | 320 - 338 °F | ASTM D3418 |
|
NatureWorks® Ingeo™ 6204D Fiber Grade PLA
NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically ..
|
|||
| Melting Point | 160 - 170 °C | 320 - 338 °F | ASTM D3418 |
|
NatureWorks® Ingeo™ 6251D Fiber Grade PLA
NatureWorks® PLA polymer 6251D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6251D is designed for spunbond products using conv..
|
|||
| Melting Point | 160 °C | 320 °F | ASTM D3418 |
|
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA
NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip..
|
|||
| Melting Point | 160 °C | 320 °F | STN EN 11357-1 |
|
Plastcom PLASTALEN® PH 52 T 20 Polypropylene reinforced with mineral filler
PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r..
|
|||
| Melting Point | 160 - 171 °C | 320 - 340 °F | MQSA 111 |
|
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer
(discontinued **)
PEARLTHANE® 12K85A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e..
|
|||
| Melting Point | 160 - 170 °C | 320 - 338 °F | Huntsman/TMA |
|
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
|
|||
| Melting Point | 160 - 168 °C | 320 - 334 °F | DSC |
|
Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF)
Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Medium ViscosityUses: Batteries; BinderAdditional Prope..
|
|||
| Melting Point | 160 °C | 320 °F | DSC |
|
Silon Tabond 2006 Adhesive Resin
Tabond 2006 is a chemically modified thermoplastic polyolefin with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated g..
|
|||
| Melting Point | 160 - 165 °C | 320 - 329 °F | DSC; ISO 3146 |
|
Borealis HC401BF Polypropylene Homopolymer
HC401BF is a polypropylene homopolymer. Applications HC401BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, package..
|
|||
| Melting Point | 160 °C | 320 °F | DSC |
|
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene
DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation..
|
|||
| Melting Point | 160 °C | 320 °F | DSC |
|
Polyram BondyRam® 1001 Maleic Anhydride modified Homo-polypropylene coupling agent
Maleic Anhydride modified Homo-polypropylene recommended for coupling of glass and other fillers in polypropylene compositesInformation provided by Polyram Ram On Ind.
|
|||
| Melting Point | 160 °C | 320 °F | |
|
Tisan TISREN® Flame Retardant (V0) Polystyrene
TISREN has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimensio..
|
|||
| Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
|
Total PPC 5946WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 5946WZ is a nucleated impact copolymer with a Melt Flow index of 75 g/10 min.TOTAL Polypropylene 5946WZ is characterized by very low warpage, improved stiffness, a..
|
|||
| Melting Point | 160 °C | 320 °F | Kofler |
|
Lubrizol Estane® 58246 Thermoplastic Polyurethane
Features: High stiffness grade with excellent chemical and oil resistance.Uses: Flat Die/Cast Film Extrusion and Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaI..
|
|||
| Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
|
Total PPC 4720XWZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4720XWZ is a nucleated impact copolymer with a Melt Flow index of 25 g/10 min.TOTAL Polypropylene 4720XWZ is characterized by improved stiffness, creep resistance,..
|
|||
| Melting Point | <= 160 °C | <= 320 °F | Peak Melting Point; ExxonMobil method |
|
ExxonMobil Escorene™ UL 00328 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00328 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applications: Compoun..
|
|||
| Melting Point | 160 °C | 320 °F | ASTM D3418 |
|
Ensinger Tecaform™ UD Blue Ultra Detectable Acetal Copolymer (POM)
TECAFORM® UD Blue is an Ultra Detectable acetal copolymer designed specifically for applications in the food industry. High speed food production lines detect particulate matter in the food product..
|
|||
| Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
|
Eurotec® Tecolen® CP10 GR15 NL PPCP, 15% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
|
Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Melting Point | 160 °C | 320 °F | ISO 11357 |
|
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
|
|||
| Melting Point | 160 °C | 320 °F | ISO 11357 |
|
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
|
|||
| Melting Point | 160 - 164 °C | 320 - 327 °F | |
|
Addcomp PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..
|
|||
| Melting Point | 160 - 165 °C | 320 - 329 °F | ATOFINA Method |
|
Total PPC 4280W Polypropylene, Impact Copolymer
ATOFINA 4280W polypropylene is a nucleated impact copolymer. 4280W has a low fluidity providing melt strength with excellent impact properties. It is nucleated for added stiffness and surface hard..
|
|||
| Melting Point | 160 °C | 320 °F | DSC; STN EN ISO 3146 |
|
Plastcom SLOVALEN PH 51 T 20 Polypropylene Homopolymer, 20% Mineral Filled
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application ..
|
|||
| Melting Point | 160 °C | 320 °F | ASTM D789 |
|
Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 160 °C | 320 °F | Crystalline, Peak; ASTM D3418 |
|
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |
|||