| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 174 °C | 345 °F | Crystallinity by DSC; ASTM D 3418 |
|
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **)
Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate..
|
|||
| Melting Point | 174 °C | 345 °F | ASTM D3418 |
|
3M Dyneon™ PVDF 1010/0001 Polyvinylidene Fluoride
(discontinued **)
Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an..
|
|||
| Melting Point | 174 - 178 °C | 345 - 352 °F | Average value: 175 °C Grade Count:5 |
|
Overview of materials for Nylon 12, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Melting Point | 174 - 184 °C | 345 - 363 °F | Average value: 177 °C Grade Count:9 |
|
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Melting Point | 174 - 178 °C | 345 - 352 °F | Average value: 175 °C Grade Count:6 |
|
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Melting Point | 174 - 186 °C | 345 - 367 °F | |
|
Indium Corp. Indalloy® 231 Sn-Zn-In-Bi Solder Alloy
Pb free solder. Zn causes high drossing; corrosion concerns.Information provided by the manufacturer, Indium Corporation.
|
|||
| Melting Point | 174 °C | 345 °F | |
|
Shakespeare MX-229 PVDF Monofilament
Outstanding resistance to weathering/UV exposure; outstanding chemical resistance; low surface energy; low COF; low moisture regain; inherent flame resistance.Information provided by Shakespeare Com..
|
|||
| Melting Point | 174 °C | 345 °F | ASTM D-3418 |
|
Saint-Gobain Norton® PVDF Fluoropolymer Film
Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from..
|
|||
| Melting Point | 174 °C | 345 °F | ASTM D3418 |
|
SK Chemicals SKYPEL G130D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® L 16 W 20 black 9995 PA12
Product Description: Grilamid L 16 W 20 is a semi-flexible low viscosity, heat stabilized PA12 injection molding grade. The main characteristics of this product are: Easy flowing?High impact streng..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® L 20 W 20 grey 9280 PA12
Product Description: Grilamid L 20 W 20 grey 9280 is a semiflexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 grey 9280 is heat stabilized. The main featur..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® L 25 W 20 PA12
Product Description: Grilamid L 25 W 20 is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 is UV and heat stabilized. The main features of Grila..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® L 25 W 20 X PA12-I
Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min |
|
Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Dry)
Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termite..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min |
|
Arkema Group Rilsan® AESN TL Nylon 12, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA12,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. Good chemical resistance. Very good ability ..
|
|||
| Melting Point | 174 °C | 345 °F | (Dry) |
|
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min |
|
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Dry)
Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min |
|
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Dry)
Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min |
|
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High..
|
|||
| Melting Point | 174 °C | 345 °F | (Dry) |
|
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Conditioned)
Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l..
|
|||
| Melting Point | 174 °C | 345 °F | (Dry) |
|
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned)
Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent...
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min |
|
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Dry)
Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to ..
|
|||
| Melting Point | 174 °C | 345 °F | (Dry) |
|
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min |
|
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
|
|||
| Melting Point | 174 °C | 345 °F | 10°C/min |
|
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid..
|
|||
| Melting Point | 174 °C | 345 °F | (Dry) |
|
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High..
|
|||
| Melting Point | 174 °C | 345 °F | ASTM D3418 |
|
Ashley Polymers Ashlene® TD930H Nylon 12
A plasticized Nylon 12 offering outstanding flexibility with superior moisture and chemical resistance, UV and heat stabilized for weatherability.Data provided by the manufacturer
|
|||
| Melting Point | 174 °C | 345 °F | Crystallinity by DSC; ASTM D 3418 |
|
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **)
Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO..
|
|||
| Melting Point | 174 °C | 345 °F | Crystallinity by DSC; ASTM D 3418 |
|
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **)
Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
|
|||
| Melting Point | 174 °C | 345 °F | Crystallinity by DSC; ASTM D 3418 |
|
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **)
Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c..
|
|||