| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 127UV BK701 Acetal Homopolymer
(Unverified Data**)
Delrin® 127UV BK701 is a high viscosity, UV stabilized acetal homopolymer. It has excellent impact strength, UV resistance and thermal stability. It is well suited for automotive interior applicati..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**)
Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 527UV BK701 Acetal Homopolymer
(Unverified Data**)
Delrin® 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvements in UV aging characteristics and ther..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® SC699 NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® SC699 is a low viscosity acetal homopolymer, lubricated, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers
|
|||
| Melting Point | >= 178 °C | >= 352 °F | |
|
Hong Kun Group HBCD Flame Retardant
Chemical name: Hexabromocyclododecane. HBCD flame retardant is used primarily in extruded (XPS) or suspension-polymerized polystyrene foam (EPS). With a stabilization package and proper processing ..
|
|||
| Melting Point | 178 °C | 352 °F | ASTM D3418 |
|
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
|
|||
| Melting Point | 178 °C | 352 °F | ASTM D3418 |
|
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® L 20 G grey 9280 PA12
Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® L 20 LM PA12
Product Description: Grilamid L 20 LM is a medium viscosity Polyamide 12 (PA12) extrusion grade. Grilamid L 20 LM is UV and heat stabilized and has been modified with a nucleation agent which result..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® L 25H FWA black 9225 PA12
Product Description: Grilamid L 25 H FWA black 9225 is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA black 9225 is designed for technical injection mould..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® L 25H FWA nat PA12
Product Description: Grilamid L 25 H FWA natural is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA natural is designed for technical injection moulded com..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® LV-15H nat PA12-GF15
Product description: Grilamid LV-15H is a 15% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptiongood dimension..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® LV-65H FWA black 9225 PA12-GF65
Product description: Grilamid LV-65H FWA black 9225 is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 100ST BK602 Acetal (POM)
(Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST BK602 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM)
(Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. P..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**)
Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)
(Unverified Data**)
Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)
(Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear ..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® PC690 NC010 Acetal (POM)
(Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare indus..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 300TE BK602 Acetal (POM)
(Unverified Data**)
Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE BK602 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® FG570 NC000 Acetal Homopolymer
Delrin® FG570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber for injection molding. It has high stiffness and low warpage. It has been developed for consideration in appl..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min |
|
Arkema Group Rilsan® BESN P40 W5 TL Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11-P,EFHL,22-003Flexible grade for tubes extrusion. Available color: milky white. Light and heat stabilized. Flame retardant agent.Fire-resistant. Flexibility. High impact str..
|
|||
| Melting Point | 178 °C | 352 °F | ASTM D3418 |
|
ALM TPE-210-S Prototyping Polymer
A thermoplastic elastomer used to produce parts with “rubber like” qualities. TPE 210-S exhibits good feature definition and infiltration with polyurethane will impart even higher toughness and ab..
|
|||
| Melting Point | 178 °C | 352 °F | 10K/min; ISO 3146 |
|
CENTROPLAST CENTROMID 12 GF 30 Polyamide 12 30% glass fiber
CENTROMID 12 GF 30 is a dimensionally stable and high strength material with good electrical insulating properties. Its applications include levers and valve parts.Information provided by CENTROPLA..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® SC631 NC010 Acetal (POM)
(Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC631 is a medium-high viscosity acetal homopolymer developed for parts requiring high precision moldi..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**)
Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform..
|
|||