| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 182 - 185 °C | 360 - 365 °F | |
|
Oceanchem Group Antioxidant 168
Molecular Formula: C42H63O3PCas No.: 31570-04-4Characteristics and Uses: This product is an excellent antioxidant namely applied to polyethylene, polypropylene, polyoxymethylene, ABS resin, PS resin..
|
|||
| Melting Point | 182 - 193 °C | 360 - 379 °F | MQSA 111 |
|
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer
(discontinued **)
PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b..
|
|||
| Melting Point | 182 - 187 °C | 360 - 369 °F | Average value: 184 °C Grade Count:8 |
|
Overview of materials for Nylon 11, Cable Sheathing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o..
|
|||
| Melting Point | 182 - 191 °C | 360 - 375 °F | |
|
Lucas-Milhaupt 60 Sn-40 Pb Tin/ Silver Solder
Applications and Characteristics:Although widely used in electronics for both manual and automatic soldering applications, it is also used in general purpose applications where fast alloy flow is d..
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D2117 |
|
Samyang Triel® 5301SP Thermoplastics Polyetherester Elastomer, Double Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5301SP is intended for double extrusion.Information provided by Samyang.
|
|||
| Melting Point | 182 °C | 360 °F | ISO 11357-1/-3 |
|
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, conditioned
Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact..
|
|||
| Melting Point | 182 °C | 360 °F | ISO 11357-1/-3 |
|
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, dry
Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact..
|
|||
| Melting Point | 182 °C | 360 °F | By DSC |
|
Toyobo PELPRENE™ P55B Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
|
|||
| Melting Point | 182 °C | 360 °F | By DSC |
|
Toyobo PELPRENE™ P55U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EA-14 Homopolymer Polypropylene, 20% Talc Filled
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EL-16 Homopolymer Polypropylene, 30% Mineral Filled; Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EQ-16 Homopolymer Polypropylene, 30% Mica Filled
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell ER-14 Homopolymer Polypropylene, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EZ-16 Homopolymer Polypropylene, 30% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EA-16 Homopolymer Polypropylene, 30% Talc Filled
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EA-18 Homopolymer Polypropylene, 40% Talc Filled
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EL-18 Homopolymer Polypropylene, 40% Mineral Filled; Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EQ-18 Homopolymer Polypropylene, 40% Mica Filled
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | 50% RH; DSC |
|
Suzhou Hipro Polymers Hiprolon® 211 ESNNHL P40 Nylon
Hiprolon® 211ESNNHL P40 is a long chain polyamide compound from bio-renewable resource. It features low density, low water absorption, high dimension stability, high cold impact resistance, high bu..
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell ER-38 Homopolymer Polypropylene, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 182 °C | 360 °F | ASTM D789 |
|
Adell EZ-18 Homopolymer Polypropylene, 40% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
|
|||