Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
Internal Method
Polimeri Europa Greenflex® MP 34 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding
Greenflex MP 34 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MP 34 combines high fluidity with high elasticity.Main Applications: Gree..
Melting Point 95.0 - 105 °C
203 - 221 °F
Fine Organics FINALUX G 785 Lubricant Additive
Applications: External lubricant for rigid PVC calendered, extruded and molded articles with Ca-Zn & Tin stabilizers, synergistic co-stabilizing properties with Ca-Zn stabilizer.Information provided..
Melting Point 95.0 - 115 °C
203 - 239 °F
Indium Corp. Indalloy 44 Bismuth Solder Alloy
Information Provided by Indium Corporation
Melting Point 95.0 - 129 °C
203 - 264 °F
Indium Corp. Indalloy 69 Bismuth-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 95.0 - 136 °C
203 - 277 °F
Indium Corp. Indalloy 76 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 95.0 - 136 °C
203 - 277 °F
Indium Corp. Indalloy 78 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 95.0 - 137 °C
203 - 279 °F
Indium Corp. Indalloy 80 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 95.0 °C
203 °F
ISO 3146
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate
Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly..
Melting Point 95.0 - 104 °C
203 - 219 °F
Indium Corp. Indalloy 57 Bismuth Solder Alloy
Information Provided by Indium Corporation
Melting Point 95.0 °C
203 °F
DSC; ASTM D3418
DuPont Bynel® 39E660 Adhesive Resin
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 95.0 °C
203 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 4208 Anhydride-Modified LDPE Adhesive Resin
Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process ..
Melting Point 95.0 °C
203 °F
ASTM D3417
DuPont Elvax® 3134SBZ Ethylene Vinyl Acetate
DuPont™ Elvax® 3134SBZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additiv..
Melting Point 95.0 °C
203 °F
ASTM D3417
DuPont Elvax® 3135XZ Ethylene Vinyl Acetate
DuPont™ Elvax® 3135XZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Applicati..
Melting Point 95.0 °C
203 °F
DSC; ASTM D3417- ISO 3146
DuPont Elvax® 650Q Ethylene Vinyl Acetate
DuPont™ Elvax® 650Q is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 650Q resins can be used for the following applications: molding, compoundin..
Melting Point 95.0 °C
203 °F
ASTM D3417- ISO 3146
DuPont Elvax® 670 Ethylene Vinyl Acetate
DuPont™ Elvax® 670 is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 670 resins can be used for the following applications: molding, compounding ..
Melting Point 95.0 °C
203 °F
TRN-14
Tipco Tipcolite® TPF 1113 - Unreinforced Thermoset Phenolic Resin, 55 mm Norton Flow with 5% Hexamine
Unreinforced Phenolic Resin having 55mm Norton Flow, in Powder FormApplications: General PurposeProcessing: General PurposeInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Melting Point 95.0 °C
203 °F
TRN-14
Tipco Tipcolite® TPF 1315 - Unreinforced Phenolic Resin having 22 mm Norton Flow with 10% Hexamine
Unreinforced Phenolic Resin having 22mm Norton Flow, in Powder FormApplications: Foundry & RefractoryProcessing: Castings & ShellsInformation provided by the Manufacturer, Tipco Industries Ltd., Ind..
Melting Point 95.0 °C
203 °F
ASTM D3418
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low..
Melting Point 95.0 °C
203 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil EXACT™ 3040 Plastomer for Extrusion Coating Applications
Product Description: Exact 3040 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monoextrusion and coextrusion coa..
Melting Point 95.0 °C
203 °F
Dow Method (DSC)
Dow AFFINITY™ PF 1146G Polyolefin Plastomer (POP)
AFFINITY™ PF 1140G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for high speed packaging applications requiring low seal initiation temperature and good machina..
Melting Point 95.0 °C
203 °F
Dow Method
Dow AMPLIFY™ EA 103 Ethylene-ethyl Acrylate (EEA)
AMPLIFY™ EA 103 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. It can be ut..
Melting Point 95.0 °C
203 °F
Upon Melting via DSC/ASTM D3418
DuPont Elvax® 3130SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Melting Point 95.0 °C
203 °F
Upon Melting via DSC/ASTM D3418
DuPont Elvax® 3134Q Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating, Casting  (discontinued **)&l
12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Melting Point 95.0 °C
203 °F
Upon Melting via DSC/ASTM D3418
DuPont Nucrel® 1207 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued
12 wt% Methacrylic Acid.Nucrel® 1207 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des..
Melting Point 95.0 °C
203 °F
Eutectic
Indium Corp. Indalloy 38 Bismuth Solder Alloy
Information Provided by Indium Corporation