Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Melting Point 200 - 220 °C
392 - 428 °F
DSC; STN EN ISO 3146
Plastcom SLOVASTER® B BT Polyethylene Terephthalate
FeaturesPBT basic type for injection moulding. Melt is characterized by outstanding fluidity, which enables injection moulding of complicated and divided products also on multiple moulds. Anisotro..
Melting Point 200 - 220 °C
392 - 428 °F
DSC; STN EN ISO 3146
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
Melting Point 200 - 220 °C
392 - 428 °F
DSC; STN EN ISO 3146
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
Melting Point 200 - 220 °C
392 - 428 °F
DSC; STN EN ISO 3146
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant
FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 BT TS PBT, basic type
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 15 FRX 5 PBT reinforced with 15% glass fibre, with flame retardant
Features: PBT with the content of 15 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 20 000/2 PBT, 20% glass fibre
FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre, excellent flow. Characterised by excellent properties also at minus temperatures like eg. modu..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 220 °C
392 - 428 °F
STN EN 11357-1
Plastcom SLOVASTYR® B BT N PBT
Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B FRN 3 LS PBT, flame retarder, light stable
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B FRN 3 PBT, flame retarder
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B GB 20 M PBT, 20% glass beads
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 220 °C
392 - 428 °F
DSC; STN EN ISO 3146
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant
FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 20 000/1 PBT, 20% glass fibre
FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticit..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 6 PBT, 6% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Melting Point 218 - 220 °C
424 - 428 °F
Average value: 219 °C Grade Count:6
Overview of materials for Nylon, Barrier Film Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Barrier Film Copolymer". Each property range of values reported is minimum and maximum values of ..
Melting Point 218 - 220 °C
424 - 428 °F
crystalline melting point; Hot Stage Microscope
Honeywell Capran® 518 LL Heat Stabilized Nylon Film  (discontinued **)
Description: Capran® 518 LL is a green tinted, heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other hig..
Melting Point 210 - 220 °C
410 - 428 °F
Huntsman/TMA
Huntsman IROGRAN® A 95 K 4977 TPU-High Temperature Performance
Polycaprolactone and ether based. Good processability and compression set. Excellent resistance to high temperatures, water, grease, and oils.. Used in seals, wheels, and rollers.Information prov..
Melting Point 200 - 220 °C
392 - 428 °F
ISO R 1218
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Conditioned
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
Melting Point 200 - 220 °C
392 - 428 °F
ISO R 1218
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
Melting Point 200 - 220 °C
392 - 428 °F
ISO R 1218
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned
Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH
Melting Point 216 - 220 °C
420 - 428 °F
Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics.
Melting Point 200 - 220 °C
392 - 428 °F
DSC; STN EN ISO 3146
Plastcom SLOVASTER® B GF 20 FRL 4 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant
FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth..
Melting Point 200 - 220 °C
392 - 428 °F
Plastcom SLOVASTER® B1 GF 30 PBT, 30% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..