| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 222 °C | 432 °F | STN EN 11357-1 |
|
Plastcom PLASTAMID® 6 BT SD PA6
Basic type PA 6 for compounding, modified for general use. Grade can contain PA 66 up to 5% and TiO2 content up to 0.25 %. Use: automotive, engineering, electrical and consumer-goods industryInforma..
|
|||
| Melting Point | 222 °C | 432 °F | STN EN 11357-1 |
|
Plastcom PLASTAMID® 6 GF 30 005 PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 30% glass fiber, used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
Lanxess Durethan® B 35 FA 000000 Nylon 6, Film Grade
PA 6, film , medium viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Applicati..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1, -3 |
|
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS.
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
Lanxess Durethan® BKV 50 H2.0 EF 000000 Nylon 6, 50% Glass Fiber
PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber
PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
Lanxess Pocan® B 3215 XF 000000 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding, improved flowability, impact modified
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance
|
|||
| Melting Point | 222 °C | 432 °F | ISO 11357 |
|
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY
Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr..
|
|||
| Melting Point | 222 °C | 432 °F | ISO 3146-C |
|
Solvay Technyl® C216V25 25% Glass Filled Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
|
|||
| Melting Point | 222 °C | 432 °F | ISO 3146-C |
|
Solvay Technyl® C218V30 30% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
|
|||
| Melting Point | 222 °C | 432 °F | ISO 11357 |
|
Solvay TECHNYL® PSB 286 PA6, DRY
Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl..
|
|||
| Melting Point | 222 °C | 432 °F | |
|
Techmer ES HiFill® TPX-PBT-98010 BN069
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C..
|
|||
| Melting Point | 222 °C | 432 °F | ISO 3146 |
|
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6
Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay.
|
|||
| Melting Point | 222 °C | 432 °F | |
|
Tisan TISLAMID® 6 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30
Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® BG-30/2 PA6-GF30
Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® BG-40 FC PA6-GF40
Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® BS PA6
Product description: Grilon BS is an unreinforced, heat stabilized standard PA6 injection molding grade with normal melt viscosity. Grilon BS has the following important properties: Good flow behavi..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® XE 5026 (BG-30 H) PA6-GF30
Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) bl..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® BG-50 PA6-GF50
Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® BK-30 PA6-GB30
Information provided by EMS Grivory
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® EB 50 H DZ PA6
Product description: Grilon EB 50 H DZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon EB 50 H DZ has the following important properties:..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® XE 5004 (BM-30/2 UV) PA666-MD30
Product description: Grilon XE 5004 is a normal viscosity PA6 injection molding grade with 30% mineral reinforcement, which is additionally UV stabilized. Grilon XE 5004 has the following important ..
|
|||
| Melting Point | 222 - 226 °C | 432 - 439 °F | 10°C/min; ISO11357 (DSC) |
|
BLUESTAR PBT 1100
PBT resin is polymerized by pure terephthalic acid (PTA) and 1,4-butanediol (1,4-BDO) through direct esterification. With well-distributed molecular weight and stable quality, PBT resin possesses go..
|
|||
| Melting Point | 222 °C | 432 °F | ISO 11357 |
|
Solvay TECHNYL® 1015CR PA6, DRY
Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re..
|
|||
| Melting Point | 222 °C | 432 °F | ISO 11357 |
|
Solvay TECHNYL® 1021ST PA6, DRY
Description: Polyamide 6, unfilled, super tough impact modified, for injection moldingAvailable in: Asia Pacific Product Applications: TECHNYL® 102ST has the highest level impact strength and balan..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® BG-50 FC PA6-GF50
Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surfac..
|
|||
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® F 50 nat 6368 PA6
Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro..
|
|||