| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 260 °C | 500 °F | STN EN 11357-1 |
|
Plastcom PLASTAMID® 66 GF 20 PA66 reinforced with glass fiber
PA66 reinforced with 20 % glass fiber, used in the automotive, engineering and electrical industry. Application: hobby tools, covers of electrotools, electromotors, cooling screws of blowers, gear w..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Plastcom SLOVAMID 66 FRC 2 PA66, basic type
FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. Used in automotive, electrical, engineering and co..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Plastcom SLOVAMID 66 GF 25 FRI 2 PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Plastcom SLOVAMID 66 Y 35 FRY 7 PA66, 35% mineral filling
FeaturesPA 66 for injection moulding, chemically reinforced with 35 % mineral filler and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /3.2 mm/ in accordance wi..
|
|||
| Melting Point | 260 °C | 500 °F | ASTM D789 |
|
PolyOne Nymax™ GF 1200 A 40 IM Black 13A Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357-3 |
|
Pasargad Polymer Peyvand Pasamid 3P-H2130B Nylon 66, 30% Glass Fiber Reinforced
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357 |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357-3 |
|
Solvay Specialty Polymers Omnix® FC-9050 Polyamide, High Performance (HPPA), 50% Glass Fiber
Omnix® FC-9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
ScanTube ETFE Tubing
Information provided by ScanTube, Inc.
|
|||
| Melting Point | 260 - 265 °C | 500 - 509 °F | |
|
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 3146 |
|
Wellman Wellamid® GF43-66/6 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
|
|||
| Melting Point | 260 °C | 500 °F | ISO 3146 |
|
Wellman Wellamid® GSF25/15-66 22L-NBK1 40% Glass Sphere/Fiber Reinforced Nylon 66
Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman.
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Akulon® S223-HG6 (Dry) 30% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Akulon® S245-C PA66
High Viscosity
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® AG-30 LF 15 PA66-(GF+Z)45
Product description: Grilon AG-30 LF 15 black 9832 is a heat stabilized, normal viscosity PA66 injection molding grade with 30% glass fibers and 15% of a combination of PTFE and silicone. Grilon AG-..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30
Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® TSS PA666
Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHi..
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Daikin NEOFLON EP-610 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
|
|||
| Melting Point | 260 °C | 500 °F | ASTM D2133 |
|
E-Polymers TEKAMID® TA210GR , 33% Glass Fiber Reinforced PA66, DAM
33% Glass Fiber reinforced, Anti EG, Anti HydrolysisInformation provided by E-Polymers Co. Ltd.
|
|||
| Melting Point | 260 °C | 500 °F | ASTM D2133 |
|
E-Polymers TEKAMID® TA210HI , High Impact Resistance PA66, DAM
High impact resistanceInformation provided by E-Polymers Co. Ltd.
|
|||
| Melting Point | 260 °C | 500 °F | ASTM D2133 |
|
E-Polymers TEKAMID® TA210L Lubricated PA66, DAM
LubricatedInformation provided by E-Polymers Co. Ltd.
|
|||
| Melting Point | 260 °C | 500 °F | ASTM D2133 |
|
E-Polymers TEKAMID® TA250G60 60% Glass Fiber Reinforced, High Modulus PA66 Resin
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60
Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory..
|
|||
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® GV-4H PA*-GF40
Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide...
|
|||
| Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
|
Addiplast Addinyl A2 W Nylon 66
High molding rateInformation provided by Addiplast.
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357-3 |
|
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Melting Point | 260 °C | 500 °F | ASTM D3417 |
|
Quantum Nylon 6/6 30% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics
|
|||
| Melting Point | 260 °C | 500 °F | |
|
Radici Radilon® A 42 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 11357-3 |
|
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
|
|||
| Melting Point | 260 °C | 500 °F | ISO 3146 |
|
BASF Ultramid® A3K Q601 PA66(Dry)
Description: Ultramid A3K Q601 is an easy flowing, injection molding grade PA66.Applications: Typical applications include fast processing high stress technical parts or electrically insulating part..
|
|||