| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 263 °C | 505 °F | ISO 11357-1,-3 |
|
Nanocyl PLASTICYL™ PA1501 Polyamide 66 - Carbon Nanotube Masterbatch
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..
|
|||
| Melting Point | 263 °C | 505 °F | |
|
Oxford Polymers Oxnilon 66-50GF 50% Glass Fiber Filled Nylon 66 for Injection Molding
50% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers.
|
|||
| Melting Point | 263 °C | 505 °F | DAM; ASTM D3418 |
|
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**)
Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers
|
|||
| Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**)
Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po..
|
|||
| Melting Point | 263 °C | 505 °F | 10°C/min; ISO 11357-1/-3 |
|
Lanxess Durethan® A 30 S 000000 Nylon 66
PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins
|
|||
| Melting Point | 263 °C | 505 °F | 10°C/min; ISO 11357-1, -3 |
|
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Melting Point | 263 °C | 505 °F | ISO 11357 |
|
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, DRY
Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of..
|
|||
| Melting Point | 263 °C | 505 °F | ISO 11357 |
|
Solvay TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY
Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH..
|
|||
| Melting Point | 263 °C | 505 °F | ISO 11357 |
|
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
|
|||
| Melting Point | 263 °C | 505 °F | ISO 11357 |
|
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, DRY
Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 7..
|
|||
| Melting Point | 263 °C | 505 °F | ISO 11357 |
|
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY
Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl..
|
|||
| Melting Point | 263 °C | 505 °F | ISO 11357 |
|
Solvay TECHNYL® A 221 PA66, DRY
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
|
|||
| Melting Point | 263 °C | 505 °F | ISO 11357 |
|
Solvay TECHNYL® A 402H1 Natural PA66, DRY
Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The ..
|
|||
| Melting Point | 263 °C | 505 °F | ASTM D3418 |
|
Samyang Tramid® 210G15 Polyamide, Reinforced
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G15 is a reinforced grade.Applications:Automotive gear level housingConnectors..
|
|||
| Melting Point | 263 °C | 505 °F | ISO 11357 |
|
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, DRY
Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co..
|
|||
| Melting Point | 263 °C | 505 °F | ISO 11357 |
|
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY
Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry..
|
|||
| Melting Point | <= 263 °C | <= 505 °F | Peak Melting Point; ExxonMobil method |
|
ExxonMobil LLDPE LL 3402.48 Blown Linear Low Density Polyethylene Resin
Product Description: LL 3402.48 is a hexane medium density polyethylene blown film grade for applications requiring high stiffness. It can also be used in cast films. Films produced from the resin e..
|
|||
| Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Minlon® 10B140 NC010 Nylon 66
(Unverified Data**)
40% Mineral Reinforced Polyamide 66Minlon 10B140 NC010 is a 40% mineral reinforced polyamide 66 for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
|
|||
| Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66
(Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL BK039B is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor..
|
|||
| Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® 70G35NOX BK309 Nylon 66
Zytel® 70G35NOX BK309 is a 35% glass reinforced, polyamide 66 resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution.Information provided by DuP..
|
|||
| Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66
Unreinforced High Viscosity Polyamide 66 Information provided by DuPont Performance Polymers
|
|||
| Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**)
33% Glass Reinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications su..
|
|||
| Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® FN714 NC010A Nylon 66
Zytel® FN714 NC010A is an impact modified, very flexible, plasticizer free polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
|
|||
| Melting Point | 263 °C | 505 °F | ASTM D789 |
|
Adell AR-18 Nylon 66, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 263 °C | 505 °F | DAM; ASTM D3418 |
|
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
|
|||
| Melting Point | 263 °C | 505 °F | DAM; ASTM D3418 |
|
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
|
|||
| Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**)
35% Glass Reinforced Heat Stabilized Laser Markable Polyamide 66 Zytel LM70G35HSLX is a 35% glass fiber reinforced heat stabilized lubricated polyamide 66 for injection molding. It is well suited fo..
|
|||
| Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**)
Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
|
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**)
Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info..
|
|||