Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 275 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio..
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146
Murtfeldt Muralen® plus + AB Polyethylene, Antibacterial
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of..
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146
Murtfeldt Muralen® Polyethylene
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of..
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial
Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp..
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction
This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan..
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146
Murtfeldt Original Material ”S”® plus + TLS Polyethylene
Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i..
Melting Point 133 - 135 °C
271 - 275 °F
DSC ISO 3146
Okulen® 1000 - REG PE Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 133 - 135 °C
271 - 275 °F
DSC ISO 3146
Okulen® 1000 - REG PE Multicoloured coarse
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 133 - 135 °C
271 - 275 °F
DSC ISO 3146
Okulen® 1000 PE-UHMW, AST
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 133 - 135 °C
271 - 275 °F
DSC ISO 3146
Okulen® 1000 PE-UHMW, Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 133 - 135 °C
271 - 275 °F
DSC ISO 3146
Okulen® 1000 PE-UHMW, UV - stabilized
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Melting Point 130 - 135 °C
266 - 275 °F
DSC ISO 3146
Okulen® 500 - REG PE Colored
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
Melting Point 130 - 135 °C
266 - 275 °F
DSC ISO 3146
Okulen® 500 - REG PE Multicoloured coarse
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
Melting Point 130 - 135 °C
266 - 275 °F
DSC ISO 3146
Okulen® 500 - REG PE Multicoloured fine
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
Melting Point 130 - 135 °C
266 - 275 °F
DSC ISO 3146
Okulen® 500 PE-HMW, Coloured
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146; DSC, 10°C/min
Quadrant EPP Cesticolor™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146; DSC, 10°C/min
Quadrant EPP Cestidur™ Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146; DSC, 10°C/min
Quadrant EPP Cestilene™ HD 1000 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146; DSC, 10°C/min
Quadrant EPP Cestilene™ HD 1000 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Melting Point 126 - 135 °C
258 - 275 °F
Average value: 130 °C Grade Count:32
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Melting Point 96.0 - 135 °C
205 - 275 °F
Indium Corp. Indalloy 74 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 125 - 135 °C
257 - 275 °F
MQSA 111
Lubrizol Advanced Materials Pearlthane® 12C75 Thermoplastic Polyurethane Elastomer
Pearlthane® 12C75 is a standard polyester based TPU supplied in form of translucent, colorless pellets, specially designed for compounds in which TPU is used as an additive. Features include low ..
Melting Point 120 - 135 °C
248 - 275 °F
DayGlo ZQ Pigments ZQ-15 Blaze Orange
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Melting Point 120 - 135 °C
248 - 275 °F
DayGlo ZQ Pigments ZQ-16 Arc Yellow
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Melting Point 120 - 135 °C
248 - 275 °F
DayGlo ZQ Pigments ZQ-17 Saturn Yellow
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Melting Point 120 - 135 °C
248 - 275 °F
DayGlo ZQ Pigments ZQ-21 Corona Magenta
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Melting Point 130 - 135 °C
266 - 275 °F
DIN 53 736
Hippe PE 1000 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Melting Point 130 - 135 °C
266 - 275 °F
DIN 53 736
Hippe PE 500 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Melting Point 130 - 135 °C
266 - 275 °F
10K/min; ISO 3146
CENTROPLAST CENTROLEN PE-HD Polyethylene high density
This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor..
Melting Point 124 - 135 °C
255 - 275 °F
Average value: 129 °C Grade Count:19
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..