| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 141 - 145 °C | 285 - 293 °F | ASTM D3418 |
|
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
|
|||
| Melting Point | 130 - 145 °C | 266 - 293 °F | ISO 3146-C |
|
FKuR Kunststoff Terralene® HD 3505 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
|
|||
| Melting Point | 130 - 145 °C | 266 - 293 °F | ISO 3146-C |
|
FKuR Kunststoff Terralene® LL 1101 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
|
|||
| Melting Point | 130 - 145 °C | 266 - 293 °F | ISO 3146-C |
|
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
|
|||
| Melting Point | 130 - 145 °C | 266 - 293 °F | ISO 3146-C |
|
FKuR Kunststoff Terralene® WF 3516 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
|
|||
| Melting Point | 130 - 145 °C | 266 - 293 °F | ISO 3146-C |
|
FKuR Kunststoff Terralene® WF 5525 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
|
|||
| Melting Point | 130 - 145 °C | 266 - 293 °F | ISO 3146-C |
|
FKuR Kunststoff Terralene® WF 6534 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
|
|||
| Melting Point | 118 - 145 °C | 244 - 293 °F | |
|
Indium Corp. Indalloy 87 Indium-Tin Solder Alloy
Information Provided by Indium Corporation
|
|||
| Melting Point | 135 - 145 °C | 275 - 293 °F | MQSA 111 |
|
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera..
|
|||
| Melting Point | 135 - 145 °C | 275 - 293 °F | MQSA 111 |
|
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer
PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp..
|
|||
| Melting Point | 125 - 145 °C | 257 - 293 °F | |
|
Struktol MAGNESIUM STEARATE
High purity stearate with low soluble salt level that reduces discoloration during processing.STRUKTOL® Magnesium Stearate is used by the rubber and plastic industries as an effective elastomer p..
|
|||
| Melting Point | 118 - 145 °C | 244 - 293 °F | |
|
Williams Advanced Alloys WS145 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
|
|||
| Melting Point | 135 - 145 °C | 275 - 293 °F | Sheath |
|
EMS-Griltech Grilon® BA 140 White Nylon 66/CoPA Bi-Component Fiber
Description: GRILON BA 140 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 135 - 145 °C. The fine count bi-component fiber guarantees an even distrib..
|
|||
| Melting Point | 135 - 145 °C | 275 - 293 °F | ISO 11357-3 |
|
Addcomp PRIEX® 25093 Maleic Anhydride Grafted PP random copolymer
Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, or mineral filled polyp..
|
|||
| Melting Point | 135 - 145 °C | 275 - 293 °F | ISO 11357-3 |
|
Addcomp PRIEX® 25097 Maleic Anhydride Grafted PP random copolymer
Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fiber, wood flour, natural fibers, multilayer films, aluminum foils, o..
|
|||
| Melting Point | 140 - 145 °C | 284 - 293 °F | |
|
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Melting Point | 140 - 145 °C | 284 - 293 °F | |
|
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
|
|||
| Melting Point | 140 - 145 °C | 284 - 293 °F | |
|
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Melting Point | 144 - 145 °C | 291 - 293 °F | |
|
BASF 2-Methyl Imidazole Flake
Formula: C4H6N2CAS: 693-98-1Description: 2-Methylimidazole or 2MI is a colorless to yellowish solid with an amine-like odor. Synonyms: 2-Methyl-1H-imidazoleApplications: Intermediate used in Pharmac..
|
|||
| Melting Point | 144 - 145 °C | 291 - 293 °F | |
|
BASF 2-Methyl Imidazole Pure
Formula: C4H6N2CAS: 693-98-1Description: 2-Methylimidazole or 2MI is a colorless to yellowish solid with an amine-like odor. Synonyms: 2-Methyl-1H-imidazolApplications: Intermediate used in Pharmac..
|
|||
| Melting Point | 140 - 145 °C | 284 - 293 °F | |
|
Arkema Group KYNAR® 2821-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..
|
|||
| Melting Point | 140 - 145 °C | 284 - 293 °F | |
|
Arkema Group KYNAR® EXAD 3000 Polyvinylidene Fluoride - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Extrusion aid, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanic..
|
|||
| Melting Point | 140 - 145 °C | 284 - 293 °F | MQSA 70 A |
|
Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane
(discontinued **)
PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperat..
|
|||
| Melting Point | 135 - 145 °C | 275 - 293 °F | Sheath |
|
EMS-Griltech Grilon® BA 140 White Nylon 66/CoPA Bi-Component Fiber
Description: GRILON BA 140 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 135 - 145 °C. The fine count bi-component fiber guarantees an even distrib..
|
|||
| Melting Point | 140 - 145 °C | 284 - 293 °F | |
|
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Melting Point | 140 - 145 °C | 284 - 293 °F | |
|
Arkema Group KYNAR® 2801-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..
|
|||