| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
|
DSM Stanyl® 46HF4130 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
|
DSM Stanyl® 46HF4130 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
|
DSM Stanyl® TE250F3 (DAM) Nylon 46 15% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
|
DSM Stanyl® TE250F9 (DAM) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TQ261F2 PA46-GF10
10% Glass Reinforced, Heat Stabilized
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TS271P4 PA46-MF20
20% Whisker Reinforced, Wear and Friction Modified
|
|||
| Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
|
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
|
DSM Stanyl® TW241F10 (COND) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TW241F3 Nylon 46-15% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperature..
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15
15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TW271F6J10 (PA46+PTFE)-GF30
30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TW275F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
|
DSM Stanyl® TW300 (DAM) Nylon 46 Heat Stabilized, Lubricated (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
|
DSM Stanyl® TW363 (DAM) Nylon 46 Heat Stabilized, Impact Modified (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50
Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30
Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab..
|
|||
| Melting Point | 295 °C | 563 °F | DIN 53 736 |
|
Hippe PA 6 Nylon 6
Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump..
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Melting Point | 295 °C | 563 °F | DIN 53765 |
|
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
|
|||
| Melting Point | 295 °C | 563 °F | DIN 53765 |
|
BASF Ultramid® KR 4350 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
|
|||
| Melting Point | 295 °C | 563 °F | DIN 53765 |
|
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Cond)
(discontinued **)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
|
|||
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||