| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 178 °C | 352 °F | ASTM D3418 |
|
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**)
Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® FG511DP is a medium viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications such ..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min |
|
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
|
|||
| Melting Point | 178 °C | 352 °F | ASTM D3418 |
|
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
|
|||
| Melting Point | 178 °C | 352 °F | ASTM D3418 |
|
UBE UBESTA® 3020X25L Rigid Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: for coating steel and aluminumInformation provided by UBE.
|
|||
| Melting Point | 178 °C | 352 °F | ASTM D3418 |
|
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12
Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron..
|
|||
| Melting Point | 178 °C | 352 °F | |
|
EMS-Griltech Grilamid® DM 10 Nylon 12 Monofilament
Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by EMS-Griltech.
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® L 20 LM PA12
Product Description: Grilamid L 20 LM is a medium viscosity Polyamide 12 (PA12) extrusion grade. Grilamid L 20 LM is UV and heat stabilized and has been modified with a nucleation agent which result..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30
Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50
Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65
Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following ..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® XE 3915 PA12-GF50
Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 127UVE RD402 Acetal (POM)
(Unverified Data**)
UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE RD402 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers pigmented red with very low ..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 300PE NC010 Acetal (POM)
(Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE NC010 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer
Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 327UVE RD402 Acetal (POM)
(Unverified Data**)
UV Stabilized Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 327UVE RD402 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers pigmented red ..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 500AF Acetal (POM)
(Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 988PA NC010 Acetal (POM)
Nucleated Low Viscosity Acetal Homopolymer with Low Screw DepositInformation provided by DuPont Performance Polymers
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® PC690 NC010 Acetal (POM)
(Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare indus..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® SC690 NC010 Acetal (POM)
(Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare indus..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® FG570 NC000 Acetal Homopolymer
Delrin® FG570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber for injection molding. It has high stiffness and low warpage. It has been developed for consideration in appl..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt..
|
|||
| Melting Point | 178 °C | 352 °F | DIN 53 736 |
|
Hippe PVDF
Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol..
|
|||
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by..
|
|||