| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
|
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
|
Plastcom SLOVASTER® B GF 20 FRK 3 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant
FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol..
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | |
|
Plastcom SLOVASTER® B PBT, basic type
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | |
|
Plastcom SLOVASTER® B1 GF 15 FRX 5 PBT reinforced with 15% glass fibre, with flame retardant
Features: PBT with the content of 15 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho..
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | |
|
Plastcom SLOVASTER® B1 GF 20 000/2 PBT, 20% glass fibre
FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre, excellent flow. Characterised by excellent properties also at minus temperatures like eg. modu..
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | |
|
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | |
|
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | |
|
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Melting Point | 200 °C | 392 °F | |
|
DuPont™ Biomax® 800C Hydro/Biodegradable Polyester
(discontinued **)
Fully degradable polymer based on PET polyester technology. It is suited for single-use products such as films for food packaging, paper coating, injection molding uses, and thermoforming. Product..
|
|||
| Melting Point | 200 - 310 °C | 392 - 590 °F | Average value: 260 °C Grade Count:44 |
|
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
|
|||
| Melting Point | 200 °C | 392 °F | ASTM D3418 |
|
Honeywell Aegis™ HCA95ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **)
Description: Aegis HCA95ZP is a medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It p..
|
|||
| Melting Point | 200 °C | 392 °F | Peak |
|
LG Chemical KEYFLEX BT 5035D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
|
|||
| Melting Point | 200 °C | 392 °F | Peak |
|
LG Chemical KEYFLEX BT GN7155F Ester Type TPE
Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical
|
|||
| Melting Point | 200 °C | 392 °F | Peak |
|
LG Chemical KEYFLEX BT HB9242D Ester Type TPE
Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
|
|||
| Melting Point | 200 °C | 392 °F | |
|
Global EPP PA 6C IMPACT Cast Polyamide 6 + Plasticizer
Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of ..
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
|
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned
Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
|
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Dry
Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Melting Point | 200 °C | 392 °F | ASTM D2117 |
|
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r..
|
|||
| Melting Point | 200 °C | 392 °F | By DSC |
|
Toyobo PELPRENE™ S1002 Polyester TPE, Ultra Heat-resistant
Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo.
|
|||
| Melting Point | 200 °C | 392 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50
Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
|
|||
| Melting Point | 200 °C | 392 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50
Product Description: Grilamid 1SVX-50H black 9288 is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile. Key properties of Grilamid 1SBVX-50H LDS ..
|
|||
| Melting Point | 200 °C | 392 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65
Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E..
|
|||
| Melting Point | 200 °C | 392 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Novamid® 2030CA PA666
Film Extrusion, Extrusion, Extrusion Grade
|
|||
| Melting Point | 200 °C | 392 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50
Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010..
|
|||
| Melting Point | 200 °C | 392 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Arnitel® UM551-V Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| Melting Point | 200 °C | 392 °F | ASTM D3418 |
|
ALM PA 850 Black Nylon 11 SLS Prototyping Polymer
Information provided by Advanced Laser Materials (ALM).
|
|||
| Melting Point | 200 °C | 392 °F | ASTM D3418 |
|
ALM PA-840-GSL Filled Nylon 12 Prototyping Polymer
Engineered for excellent mechanical properties, part definition and surface finish.Stabilized against thermal degradation resulting in little or no scrap material, with typical virgin refresh rates ..
|
|||
| Melting Point | 200 °C | 392 °F | 10°C/min; ISO 11357-1/-3 |
|
Barlog Plastics KEBAFLEX P D55.1 Polyester-Elastomer, Shore D55
TPC-ETInformation provided by BARLOG plastics GmbH.
|
|||
| Melting Point | 200 - 220 °C | 392 - 428 °F | |
|
Plastcom SLOVASTER® B2 BT PBT, basic type
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
|
|||
| Melting Point | 200 °C | 392 °F | 10°C/min; ISO 11357-1/-3 |
|
EMS-Grivory Grivory® BM 20 SBG PA*
Product description: Grilon BM 20 SBG is a lactam free multipolyamide. Grilon BM 20 SBG has the following features: Lactam freeGood transparency and glossGood flexibility and toughnessVery good ther..
|
|||