| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | |
|
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre
Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi..
|
|||
| Melting Point | 223 °C | 433 °F | ISO 3146 |
|
PolyOne Bergamid™ B650 Mi10 Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Melting Point | 223 °C | 433 °F | ISO 3146 |
|
PolyOne Bergamid™ B700 UF black Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Crastin® CE15330 BK010 PBT
(Unverified Data**)
Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..
|
|||
| Melting Point | 223 °C | 433 °F | ISO 11357-1/-3 |
|
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade
(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedAs of 1 September 2015, Bayer MaterialScience was separated..
|
|||
| Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Crastin® CE15315 BK010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0..
|
|||
| Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Crastin® CE15330 BK010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V..
|
|||
| Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
|
DuPont Performance Polymers Crastin® SK692FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by ..
|
|||
| Melting Point | <= 223 °C | <= 433 °F | Peak Melting Point; ExxonMobil method |
|
ExxonMobil LDPE LD 258 Low Density Polyethylene Resin (European Grade)
Product Description: LD 258 is a LDPE extrusion coating grade, having superior organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers. The developme..
|
|||
| Melting Point | <= 223 °C | <= 433 °F | Peak Melting Point; ExxonMobil method |
|
ExxonMobil LDPE LD 368ON Low Density Polyethylene Resin
Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according..
|
|||
| Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
|
Eurotec® Tecomid® NB40 GR20 NL XA60 PA6, 20% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
|
Eurotec® Tecomid® NB40 GR50 NL IL PA6, 50% glass fiber reinforced, impact modified, natural
Information provided by Eurotec®
|
|||
| Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
|
Eurotec® Tecomid® NB40 KK30 NL PA 6 30% glass fiber/mineral reinforced, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
|
Eurotec® Tecomid® NB50 NL IT PA6, impact modified, super tough, natural, extrusion grade
Information provided by Eurotec®
|
|||
| Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
|
Eurotec® Tecomid® NB40 GR25 NL PA 6 25% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Melting Point | 223 °C | 433 °F | ASTM Test |
|
BASF Ultradur B 4300 G2 BK5110 10% Glass Filled PBT
Ultradur B 4300 G2 BK5110 is a pigmented black, easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.
|
|||
| Melting Point | 223 °C | 433 °F | ASTM Test |
|
BASF Ultradur B 4300 G3 15% Glass Filled PBT
Ultradur B 4300 G3 is an easy flowing injection molding PBT with 15% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.
|
|||
| Melting Point | 223 °C | 433 °F | ASTM Test |
|
BASF Ultradur B 4300 G6 LS BK15073 30% Glass Filled PBT
mt
|
|||
| Melting Point | 223 °C | 433 °F | 10 K/min |
|
BASF Ultradur B 4300 G6 LS High Speed BK15045 30% Glass Filled PBT |
|||
| Melting Point | 223 °C | 433 °F | ASTM Test |
|
BASF Ultradur B 4520 BK00110 PBT
Ultradur B 4520 BK00110 is a medium viscosity, pigmented black, rapidly freezing injection molding grade.
|
|||
| Melting Point | 223 °C | 433 °F | ISO 11357-1/-2 |
|
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT
Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation..
|
|||
| Melting Point | 223 °C | 433 °F | ISO 11357-1/-2 |
|
BASF Ultradur® B 4520 High Speed PBT
Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF
|
|||
| Melting Point | 223 °C | 433 °F | ASTM Test |
|
BASF Ultradur B 4300 G6 BK5110 30% Glass Filled PBT
Ultradur B 4300 G6 BK5110 is an easy flowing, pigmented black, injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.
|
|||
| Melting Point | 223 °C | 433 °F | 10 K/min |
|
BASF Ultradur S 4090 G4 BK5110 20% Glass Filled PBT
Ultradur S 4090 G4 BK5110 is a 20% glass reinforced, pigmented black PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkag..
|
|||
| Melting Point | 223 °C | 433 °F | 10 K/min |
|
BASF Ultradur S 4090 G6 LS BK15077 30% Glass Filled PBT |
|||
| Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
|
Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
|
Eurotec® Tecomid® NB40 KK30 NL IL PA 6 30% glass fiber/mineral reinforced, impact modified, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
|
Eurotec® Tecomid® NB40 NL E PA6, unfilled, natural
Information provided by Eurotec®
|
|||
| Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
|
Eurotec® Tecomid® NB40 NL RM PA 6 low friction and wear
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
|
Gromax PBT 1100-211MB