| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 254 °C | 489 °F | ASTM D3418 |
|
Nylene® PA6/6 Mineral Filled 6440 HS Nylon 6/6
34% Mineral Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
|
|||
| Melting Point | 254 °C | 489 °F | |
|
Techmer ES HiFill® PET GF/M35 35% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Melting Point | 254 °C | 489 °F | |
|
Polyram RamSter PE301G6 PET, 30% Glass Fiber
30% Glass-fiber reinforced, heat stabilized PET for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Melting Point | 254 °C | 489 °F | ASTM D789 |
|
Diamond Polymers NYLON 66 Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Melting Point | 254 °C | 489 °F | DSC |
|
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® ADS Polyester Film, 500 Gauge
Mylar® ADS is a heat stabilized, low shrinkage film with good web handling properties. Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm)Also available in 285 GaugeInformation provided by..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® C Polyester Film, 14 Gauge
Mylar® Type C films are available in a wide range of generally thinner gauges (typically 10 through 92) that offer excellent electrical properties, combined with superior strength and dimensional s..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® CL Polyester Film, 100 Gauge
Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® D804 Polyester Film, 92 Gauge
Mylar® D804 is a super clear, biaxially oriented, co-extruded polyester film, available in 60, 75 and 92 gauge. Mylar® D804 is two-side pretreated for printing and adhesive lamination. Approvals: ..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® EB31 Polyester Film, 92 Gauge
Mylar® EB31 is a smooth, matte polyester film. It does not contain any plasticizers. General Product Info: Mylar® EB31 has low haze and intermediate gloss. This offers more realistic colors and cl..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® EL Polyester Film, 400 Gauge
Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® EL Polyester Film, 75 Gauge
Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® LJP Polyester Film, 275 Gauge
Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® LJP Polyester Film, 650 Gauge
Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® M577 Polyester Film, 48 Gauge
Mylar® Type M577 is a tough, transparent film. A rough surface provides ease of handling, good adhesion, and processability.General Product Info: Mylar® Type M577 film has balanced tensile propert..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® MO21 Polyester Film, 900 Gauge
Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge
Product Description: Mylar® RB42AF is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer and polyvinylidene chloride (PVdC) layer on the opposite side. ..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® RSX Polyester Film, 175 Gauge
Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® RSX951 Polyester Film, 140 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® RSX951 Polyester Film, 48 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® S1 Polyester Film, 25 Gauge
Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 300 Gauge
Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin..
|
|||
| Melting Point | 254 °C | 489 °F | DSC |
|
DuPont Teijin Films Mylar® A Polyester Film, 300 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
|
|||
| Melting Point | 254 °C | 489 °F | DSC |
|
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® HR951 Polyester Film, 92 Gauge
Mylar® HR951 is a one-side release coated polyester film with good handling properties and clarity. It has been developed for use in various industrial applications.Information provided by DuPont.
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® MDA Polyester Film, 92 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
|
|||
| Melting Point | 254 °C | 489 °F | ASTM D789 |
|
Chem Polymer Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced
A 25% mineral reinforced, 15% glass fiber reinforced nylon 66 offering excellent rigidity, dimensional stability and tensile strength with improved warpage control in large area parts.Data provided ..
|
|||
| Melting Point | 254 °C | 489 °F | ASTM D3418 |
|
Ashley Polymers Ashlene® 526 Nylon 66
High impact Nylon 66 with good stiffness and good low temperature properties for injection molding. Values shown are for Natural. Colors may change some properties.Data provided by the manufacture..
|
|||
| Melting Point | 254 °C | 489 °F | ASTM D789 |
|
Chem Polymer Chemlon 104-13 G Nylon 66, 13% Glass Fiber Reinforced
A toughened, 13% glass fiber reinforced nylon 66 exhibiting improved toughness and ductility, especially dry as molded.Data provided by the manufacturer, Chem Polymer.
|
|||
| Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
|
DuPont Teijin Films Mylar® S2 Polyester Film, 1000 Gauge
Mylar® S2 is a slightly hazy film designed for use in the production of drumheads. It has low haze, excellent impact resistance, and balanced physical properties, resulting in consistent tonal qual..
|
|||