| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 240 - 260 °C | 464 - 500 °F | SABIC (IRC0053) |
|
SABIC HC 050 Amorphous Polyethylene Terephthalate
Product Description: HC 050 is an amorphous, low molecular weight thermoplastic PET made by a continuous melt-phase polymerization process.Characteristics: HC 050 is a specially formulated amorpho..
|
|||
| Melting Point | 240 - 260 °C | 464 - 500 °F | SABIC (IRC0053) |
|
SABIC HC100 Crystalline Polyethylene Terephthalate
Product Description: HC100 is a crystalline, high molecular weight thermoplastic polymer made by a continuous melt-phase polymerization process followed by solid-state polymerization.Characteristic..
|
|||
| Melting Point | 220 - 260 °C | 428 - 500 °F | |
|
Plastcom SLOVAMID 6/66 CF 30 PA6/66, 30% carbon fibre
FeaturesPA 6/66 for injection moulding, chemically strengthened with 30% of carbon fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-..
|
|||
| Melting Point | 248 - 260 °C | 478 - 500 °F | Average value: 252 °C Grade Count:5 |
|
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep..
|
|||
| Melting Point | 220 - 260 °C | 428 - 500 °F | Average value: 226 °C Grade Count:25 |
|
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
|
|||
| Melting Point | 200 - 260 °C | 392 - 500 °F | Average value: 234 °C Grade Count:3 |
|
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
|
|||
| Melting Point | 214 - 260 °C | 418 - 500 °F | Average value: 222 °C Grade Count:41 |
|
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Melting Point | 179 - 260 °C | 354 - 500 °F | |
|
Indium Corp. Indalloy 142 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
|
|||
| Melting Point | 252 - 260 °C | 486 - 500 °F | |
|
Indium Corp. Indalloy 143 Lead Solder Alloy
Information Provided by Indium Corporation
|
|||
| Melting Point | 240 - 260 °C | 464 - 500 °F | |
|
Indium Corp. Indalloy® 10 Pb-In Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
|
|||
| Melting Point | 225 - 260 °C | 437 - 500 °F | 10°C/min; ISO 11357-1, -3 |
|
Lanxess Pocan® A 3121 901510 PBT+ASA, 20% Glass Fiber
PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS.
|
|||
| Melting Point | 225 - 260 °C | 437 - 500 °F | 10°C/min; ISO 11357-1/-3 |
|
Lanxess Pocan® T 3150 XF 000000 PBT + PET, 55% Glass Fiber
PBT+PET, 55% glass fibers, injection molding, improved flowability, low tendency to warp, increased temperature peak load, increased strength and increased modulus
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | |
|
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | |
|
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | |
|
Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | |
|
Tisan TISLAMID® 66 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | |
|
Tisan TISLAMID® 66 Flame Retardant (V0). Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | |
|
Tisan TISLAMID® 66 Impact Modified Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Melting Point | 250 - 260 °C | 482 - 500 °F | |
|
Daikin NEOFLON NP-130 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka..
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | ASTM E794-85 |
|
DuPont Teijin Films Melinex® ST328 Polyester Film, 1400 Gauge
Melinex® ST328 is an exceptionally white, opaque film with a satin finish. It is pretreated on both surfaces to promote adhesion to a wide range of solvent-based and UV-curable graphics inks and va..
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | ASTM E794-85 |
|
DuPont Teijin Films Melinex® 539 Polyester Film, 370 Gauge
Melinex® 539 is a two sided treated grade of clear film for applications where freedom from static is required. Its main use is as a montage "foil" in the production of printing plates. Melinex® 5..
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | ASTM E794-85 |
|
DuPont Teijin Films Melinex® 539 Polyester Film, 700 Gauge
Melinex® 539 is a two sided treated grade of clear film for applications where freedom from static is required. Its main use is as a montage "foil" in the production of printing plates. Melinex® 5..
|
|||
| Melting Point | 255 - 260 °C | 491 - 500 °F | ASTM E794-85 |
|
DuPont Teijin Films Melinex® 542 Polyester Film
Melinex® 542 is a slightly hazy film with an adhesion promoting pretreatment on both sidesGeneral Product Info: The pretreatment enables numerous solvent and UV inks and lacquers to be coated with ..
|
|||
| Melting Point | 215 - 260 °C | 419 - 500 °F | Average value: 221 °C Grade Count:102 |
|
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Melting Point | 222 - 260 °C | 432 - 500 °F | Average value: 251 °C Grade Count:8 |
|
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
|
|||
| Melting Point | 254 - 260 °C | 489 - 500 °F | Average value: 257 °C Grade Count:5 |
|
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
|
|||
| Melting Point | 221 - 260 °C | 430 - 500 °F | Average value: 246 °C Grade Count:3 |
|
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
|
|||
| Melting Point | 225 - 260 °C | 437 - 500 °F | Average value: 247 °C Grade Count:22 |
|
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
|
|||
| Melting Point | 225 - 260 °C | 437 - 500 °F | 10°C/min; ISO 11357-1/-3 |
|
Lanxess Pocan® TP 740-201 000000 PBT + ASA, 20% Glass Fiber
(discontinued **)
PBT+ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finish
|
|||