Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 84.2 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Melting Point 29.0 - 30.0 °C
84.2 - 86.0 °F
BASF N-Methylacetamide
Formula: C2H7NOCAS: 79-16-3Description: N-Methylacetamide is a colorless solid with a faint amine-like odor. It is fairly soluble with water and other organic solvents. Synonyms: Mono-N-methylaceta..
Melting Point 29.0 - 48.0 °C
84.2 - 118 °F
BASF Piperazine 68%
Formula: C4H10N2CAS: 110-85-0Description Piperazine 68% is a colorless to yellow hot molten with an amine-like odor. It is miscible in water.Synonyms: 1,4-Diazacyclohexane, 1,4-Piperazine, Hexahydr..