Polymer Property : Annealing Point = 1000 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Annealing Point 540 °C
1000 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Schott Glass 8651 Sealing Glass
Tungsten sealing glass Power diodesInformation provided by SCHOTT AG.
Annealing Point 540 °C
1000 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Schott ILLAX® Amber Pharmaceutical Glass
Amber Glass Pharmaceutical primary packaging for oralia and solid dosageInformation provided by SCHOTT AG.