| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 0.146 J/g-°C | 0.0349 BTU/lb-°F | Solid |
|
Indium Corp. Indalloy 160-190 Fusible Bismuth Alloy
Information Provided by Indium Corporation
|
|||
| Specific Heat Capacity | 0.146 J/g-°C | 0.0349 BTU/lb-°F | Solid |
|
Indium Corp. Indalloy® 158 Bi-Pb-Sn-Cd Solder Alloy
Lowest melting point solder. Good fusible alloy used for lens blocking.Information provided by the manufacturer, Indium Corporation.
|
|||