Polymer Property : Specific Heat Capacity = 0.0350 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.146 J/g-°C
0.0350 BTU/lb-°F
Liquid
AIM 47 Fusible Bismuth Alloy
Uses: low-temperature solder; fixturing delicate parts for machining; lens blocking; proof casting of cavities; dental models; fusible element in safety devices and alarms; radiation blocking for x-..
Specific Heat Capacity 0.146 J/g-°C
0.0350 BTU/lb-°F
Solid
AIM 47 Fusible Bismuth Alloy
Uses: low-temperature solder; fixturing delicate parts for machining; lens blocking; proof casting of cavities; dental models; fusible element in safety devices and alarms; radiation blocking for x-..