Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.335 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 80.0 °C
0.335 BTU/lb-°F
<br>@Temperature 176 °F
DSC
Eastman Heatwave CF746 Polymer &nbsp;(discontinued **)
Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 ..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 80.0 °C
0.335 BTU/lb-°F
<br>@Temperature 176 °F
ASTM E1269
Eastman Vitiva PC715 PET &nbsp;(discontinued **)
Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damagi..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 100 °C
0.335 BTU/lb-°F
<br>@Temperature 212 °F
ASTM E1269
Eastman 9921 PET Film &nbsp;(discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 100 °C
0.335 BTU/lb-°F
<br>@Temperature 212 °F
ASTM E1269
Eastman 9921 PET Injection Molded &nbsp;(discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 80.0 °C
0.335 BTU/lb-°F
<br>@Temperature 176 °F
ASTM E1269
Eastman 9921P PET Film &nbsp;(discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 80.0 °C
0.335 BTU/lb-°F
<br>@Temperature 176 °F
ASTM E1269
Eastman CB11E PET &nbsp;(discontinued **)
VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 80.0 °C
0.335 BTU/lb-°F
<br>@Temperature 176 °F
ASTM E1269
Eastman CB12 PET &nbsp;(discontinued **)
Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
Average value: 1.40 J/g-°C Grade Count:4
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Specific Heat Capacity 1.40 - 1.50 J/g-°C
0.335 - 0.359 BTU/lb-°F
Average value: 1.45 J/g-°C Grade Count:4
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8)
See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12)
See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 80.0 °C
0.335 BTU/lb-°F
<br>@Temperature 176 °F
DSC
Eastman Eastar A150 Copolyester, Film
Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)
Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade.
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Dry)
Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability.
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
IEC 1006
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 100 °C
0.335 BTU/lb-°F
<br>@Temperature 212 °F
ASTM E1269
Eastman 5214A PET &nbsp;(discontinued **)
Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe..
Specific Heat Capacity 1.40 J/g-°C
<br>@Temperature 100 °C
0.335 BTU/lb-°F
<br>@Temperature 212 °F
ASTM E1269
Eastman 9921W PET Film &nbsp;(discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF