| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | |
|
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | |
|
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products
(discontinued **)
ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and ..
|
|||
| Specific Heat Capacity | 1.17 - 1.90 J/g-°C | 0.280 - 0.454 BTU/lb-°F | Average value: 1.30 J/g-°C Grade Count:53 |
|
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | |
|
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade
Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft..
|
|||
| Specific Heat Capacity |
1.17
J/g-°C @Temperature 1100 °C |
0.280
BTU/lb-°F @Temperature 2010 °F |
|
|
Zircar Ceramics ASB-2600 Alumina-Silica Blanket
Useful to temperatures of 1400°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics.
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | ASTM D2766 |
|
Covestro Makrolon® 2658 Polycarbonate, Injection Grade
Easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer M..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | ASTM D2766 |
|
Covestro Makrolon® 2805 Polycarbonate, Injection Grade
Medium flowing injection molding grade with easy mold release, Makrolon grade 2858 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | |
|
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | |
|
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® C Polyester Film, 48 Gauge
Mylar® Type C films are available in a wide range of generally thinner gauges (typically 10 through 92) that offer excellent electrical properties, combined with superior strength and dimensional s..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® EL Polyester Film, 48 Gauge
Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® EL21 Polyester Film, 1000 Gauge
Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® MDA Polyester Film, 1200 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® MLBT Polyester Film, 48 Gauge
Product Description: Mylar® MLBT is a clear, one side corona treated polyester film suitable for flexible packaging, printing and laminations. It is also the film of choice for approved medical end..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® RSX Polyester Film, 400 Gauge
Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® D804 Polyester Film, 60 Gauge
Mylar® D804 is a super clear, biaxially oriented, co-extruded polyester film, available in 60, 75 and 92 gauge. Mylar® D804 is two-side pretreated for printing and adhesive lamination. Approvals: ..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® EB11 Polyester Film, 48 Gauge
Mylar® EB11 is a low gloss polyester film with a matte surface. It is typically used as a carrier film. It is commercially available in nominal 48 - 300 gauge. General Product Info: Mylar® EB11 is..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® M813 Polyester Film, 48 Gauge
Mylar® M813 is a clear, pretreated base film with high gloss, low haze, and excellent processability. It is a one side pre-treated polyester designed for improved ink adhesion and may be suitable f..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® MDA Polyester Film, 300 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® MDA Polyester Film, 48 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® MLB Polyester Film, 48 Gauge
Product Description: Mylar® MLB is an uncoated, transparent, polyester film designed for use as a component of a lamination structure and may be suitable for use in medical applications. Mylar® ML..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | Typical Mylar® |
|
DuPont Teijin Films Mylar® MDA Polyester Film, 200 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
|
|||
| Specific Heat Capacity | 1.17 J/g-°C | 0.280 BTU/lb-°F | ASTM C351 |
|
SABIC Innovative Plastics Lexan® 3412R PC
20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added.
|
|||
| Specific Heat Capacity | 1.17 - 1.51 J/g-°C | 0.280 - 0.360 BTU/lb-°F | DSC |
|
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||