| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | ISO 11357-1 |
|
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | ISO 11357-1 |
|
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
|
Permabond ET505 Epoxy Resin
PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
|
Lucite International Elvacite ® 2697 Acrylic Resin
Elvacite® 2697 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. Elvacite® 2697 is useful in clear, translucent or pigmented metal lacquers. It is a fast dissolvi..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | ASTM E1356 |
|
SK Chemicals SKYTHANE® US210 Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | Ultimate Tg; TMA |
|
Tra-Con Tra-Bond 516H02 Fiber Optic Adhesive
TRA-BOND 516H02 is a low viscosity, room temperature or low temperature curing fiber optic adhesive with good stress relief, high adhesion, and low shrinkage upon cure. TRA-BOND 516H02 contains very..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | Ultimate Tg |
|
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive
TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | Ultimate Tg |
|
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive
TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste s..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
|
Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
|
Loctite® Output™ 315 Acrylic Adhesive
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | ETM 300-90 |
|
ExxonMobil ESCOREZ™ 1102 (Americas) Petroleum Hydrocarbon Resin
Aliphatic hydrocarbon resin which is designed for use in a varity of applicaitons.Availability: Central America, North America and South AmericaInformation provided by ExxonMobil Chemical
|
|||
| Glass Transition Temp, Tg | >= 50.0 °C | >= 122 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
|
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy
Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..
|
|||
| Glass Transition Temp, Tg | >= 50.0 °C | >= 122 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
|
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy
Material Description: A two component, black colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..
|
|||
| Glass Transition Temp, Tg | >= 50.0 °C | >= 122 °F | |
|
Epoxy Technology EPO-TEK® B9021-1 Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
|
|||
| Glass Transition Temp, Tg | >= 50.0 °C | >= 122 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min |
|
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy
Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology
|
|||
| Glass Transition Temp, Tg | >= 50.0 °C | >= 122 °F | Post-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min |
|
Epoxy Technology EPO-TEK® OG178 UV Cure Optical Epoxy
Material Description: A single component, UV/visible shifted light curable epoxy, designed for adhesive, sealing, coating and encapsulating applications found in semiconductor, electro-optics, fiber..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | dry, dynamic; DIN 53 736 |
|
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced
These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | DAM; 10°C/min; ISO 11357-1/-2 |
|
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
|
BCC Products BC 100 Medium Cyanoacrylate Adhesive
BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | |
|
3M Scotchkote™ 162PWX Epoxy Coating
3M Scotchkote Epoxy Coating 162PWX is a 100% solid two-part epoxy coating that has been specifically developed for the long term protection of drinking water pipelines, storage and process tanks or ..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | TM R050-25 |
|
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin
Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate ..
|
|||
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | TM R050-25 |
|
Resinlab® EP1305LV Clear Epoxy Casting Resin
Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..
|
|||