| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | 148 °C | 298 °F | DMA; without post-cure |
|
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4503 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | DMA; without post-cure |
|
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | DSC |
|
Gharda Chemicals GATONE™ 5400 PEEK, Medium Viscosity Grade
(discontinued **)
Medium viscosity grade for extrusion and injection moldingCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellent mechanical prope..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | DSC |
|
Gharda Chemicals GATONE™ 5600 PEEK, Low Viscosity Grade
(discontinued **)
Low viscosity. grade for injection molding of thin sections & complex partsCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellen..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | DSC |
|
Gharda Chemicals GATONE™ PEEK, 30% Glass Reinforced
(discontinued **)
GATONE™ PEEK grades with glass fiber reinforcements ranging from 10- 40 % are available in natural or desired colors. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | DSC |
|
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced
(discontinued **)
GATONE™ PEEK grades with carbon fiber reinforcements ranging from 10- 40 % are available in natural or desired color. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | ASTM D3482 |
|
Gharda Chemicals GATONE™ 5700 Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | ASTM D3482 |
|
Gharda Chemicals GATONE™ 5630GF Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | ASTM D3482 |
|
Gharda Chemicals GATONE™ 5330FC Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | ASTM D3482 |
|
Gharda Chemicals GATONE™ 5630FC Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 2405 Polycarbonate, Injection Grade
Very easy flowing injection molding grade with easy mold release, Makrolon grade 2458 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Very easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officia..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
Very easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Ba..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | 10°C/min; ISO 11357-1,-2 |
|
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 2658 Polycarbonate, Injection Grade
Easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer M..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | 10°C/min; ISO 11357-1,-2 |
|
Covestro Makrolon® 2800 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | ISO 11357-1/-2 |
|
Covestro Makrolon® 2806 Polycarbonate
ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | ISO 11357-1/-2 |
|
Covestro Makrolon® 3103 MAS157 Polycarbonate
ISO 7391-PC,EL,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityUV stabilizedAvailable in color code 550115 onlySolid sheetCorrugated sheetPreprocessingMax. Water conte..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 6385 Polycarbonate, Injection Grade
Low viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 6557 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding grade with easy mold release, UV-stabilized.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer A..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 8035 Polycarbonate
High viscosity extrusion and injection molding grade with 30% short glass fibers and easy mold release, low anisotropy, for stiff moldings requiring good dimensional stability.Information provided b..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 8325 Polycarbonate
High viscosity injection molding and extrusion grade with 20% standard glass fibers and easy mold release, high strength and stiffness.Information provided by Bayer.As of 1 September 2015, Bayer Mat..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® 9425 Polycarbonate
High viscosity, flame retardant extrusion and injection molding grade with 20% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer MaterialS..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® AL 2647 Polycarbonate, Automotive Lens Injection Grade
Easy flowing injection molding grade, UV-stabilized, easy mold release agent.Applications: Automotive lens applications, fulfills U.S. specification SAE J 576C.Information provided by Bayer.As of 1 ..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® KU 1-1243 Polycarbonate, UV-Stabilized
Pseudoplastic behavior and high viscosity extrusion grade with UV stabilizer and easy mold release, special grade for twin-wall sheet.Information provided by Bayer.As of 1 September 2015, Bayer Mate..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® LQ 2647 Polycarbonate, UV-Stabilized
UV-stabilized injection molding grade with easy mold release, suitable for spectacle glasses (LQ = Lens Quality).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
|
Covestro Makrolon® KU 1-1216 Polycarbonate, UV-Stabilized
UV-stabilized injection molding grade, good flow, suitable for spectacle glasses (LQ = Lens-Quality).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Ba..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | ASTM D3482 |
|
Gharda Chemicals GATONE™ 5330GF Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Glass Transition Temp, Tg | 148 °C | 298 °F | ASTM D3482 |
|
Gharda Chemicals GATONE™ 5330CF Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||