Thermal Properties Metric English Comments
Glass Transition Temp, Tg 180 - 190 °C
356 - 374 °F
TMA; IPC-TM-650 2.4.24
Rogers Corporation Theta® MCL-HE-679G Laminate, GHA-679G Prepreg Halogen-Free, Low Dielectric Constant, High heat Resistant Multi-Layer Circuit Material
Theta® circuit materials are halogen free and have good dielectric characteristics suitable for high speed digital applications. Theta materials, in part due to their superior heat resistance, hav..
Glass Transition Temp, Tg 180 °C
356 °F
Laminate; standard cure
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 180 °C
356 °F
Laminate; standard cure
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 180 °C
356 °F
Laminate; standard cure
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 3k 5HS Carbon Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 180 °C
356 °F
Laminate; standard cure
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 180 °C
356 °F
Laminate; standard cure
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Glass Transition Temp, Tg 180 °C
356 °F
TMA; IPC-TM-650.2.4.24c
Park Electrochemical Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg
The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature..
Glass Transition Temp, Tg 180 °C
356 °F
Midpoint; ISO 11357
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
Glass Transition Temp, Tg 180 °C
356 °F
Tg
Industrial Laminates/Norplex MC511A Glass Fabric
Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures ar..
Glass Transition Temp, Tg 180 °C
356 °F
Tg
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate
Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con..
Glass Transition Temp, Tg 180 °C
356 °F
Polyplastics TOPAS® 6017 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade)
Possesses the highest heat resistance among cyclic olefin-type resins.Information provided by PolyPlastics.
Glass Transition Temp, Tg 180 °C
356 °F
DMA
Hexcel® HexPly® EH25 180°C Curing Epoxy Matrix
HexPly® EH25 is a high performance, tough 180°C curing matrix for us in aerospace primary structures. HexPly® EH25 is a self-extinguishing epoxy resin with controlled flow. HexPly® EH25 prepregs..
Glass Transition Temp, Tg 180 °C
356 °F
TMA; IPC-TM-650.2.4.24c
Park Electrochemical Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg
The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature..
Copyright © lookpolymers.com All Rights Reserved