| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | ASTM D3417 |
|
NatureWorks® Ingeo™ 3801X Injection Grade PLA
Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Permabond ET510 Epoxy Resin
PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Permabond ET536 Epoxy Resin
PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Permabond ET538 Epoxy Resin
PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Lucite International Elvacite ® 2028 Acrylic Resin
Elvacite® 2028 is a low molecular weight methacrylate copolymer. It is unique in its broad compatibility and solubility. Elvacite® 2028 is designed for flexographic inks, general - purpose lac..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Styron XZ 92077.01 Functionalized SB
Performance Features: Excellent fiber bonding, medium stiff hand, good filler acceptanceApplications: Fiber Binding, Glass Fiber Binding and NonwovensEuropeInformation provided by Styron
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Styron XZ 91875.00 Functionalized SB
Performance Features: Optimized for melamine and reactive resin based systemsApplications: Fiber Binding, Glass Fiber Binding and NonwovensEuropeInformation provided by Styron
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Unitika elitel UE3210 Polyester, Pellet
Medium Tg, standard resin, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bi..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Unitika elitel UE3215 Polyester, Pellet
Low molecular weight type UE3210UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bin..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Unitika elitel UE3300 Polyester, Flake
Low molecular weight type UE3210, High OH type, Branched & highly crosslinkedUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications fro..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | Ultimate Tg |
|
Tra-Con Tra-Bond 2111 Rigid Epoxy Staking Compound
TRA-BOND 2111 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | Ultimate Tg |
|
Tra-Con Tra-Bond F113 High Impact Optically Clear Epoxy Adhesive
TRA-BOND F113 is an optically clear, low viscosity, high impact epoxy adhesive developed for bonding and small volume potting of plastic or glass optical fibers, lenses, and prisms, LED displays, an..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | Ultimate Tg |
|
Tra-Con Tra-Coat OPL6E Low Viscosity Adhesive
Information provided by Tra-Con Inc.
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | Ultimate Tg |
|
Tra-Con Tra-Duct 2979 Microelectronic Conductive Epoxy Adhesive
TRA-DUCT 2979 is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid t..
|
|||
| Glass Transition Temp, Tg | 45.0 - 48.0 °C | 113 - 118 °F | Dry Polymer |
|
Eastman Eastman F-Cat HC Polyester Concentrate
Applications:Carpet FibersProduct Description: Eastman Polymer F-Cat HC is a polyester concentrate intended to impart cationic dyeable properties to extruded polyester fibers. The primary applicat..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | ETM E-90 |
|
ExxonMobil ESCOREZ™ 2184 (Europe) Petroleum Hydrocarbon Resin
Aromatic modified aliphatic hydrocarbon resin giving excellent compatibility with natural and most synthetic rubbers and with EVA copolymers. It is especially useful as a single tackifier for natura..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | ETM 300-90 |
|
ExxonMobil Escorez™ 2203LC (AM & EU) Tackifying Resin
Product Description: Escorez™ 2203LC is a premium aromatic modified aliphatic hydrocarbon resin with a narrow molecular weight distribution. It is characterized by low color and low volatility. It..
|
|||
| Glass Transition Temp, Tg | >= 45.0 °C | >= 113 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
|
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy
Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Epoxyset Epoxibond EB-109M-4 Unfilled Epoxy Adhesive
A two-component, unfilled, flexible epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-109M-4 puts low stress on fragile parts a..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Atom Adhesives AA-BOND F113 Epoxy Adhesive
AA-BOND F113 is an Optically Clear, low viscosity , High impact epoxy adhesives developed for bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, an..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | |
|
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive
AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | Ultimate Tg |
|
Tra-Con Tra-Bond 2138 Easy-Flow No-Sag Epoxy Adhesive
TRA-BOND 2138 epoxy adhesive is an easy-to-apply, room temperature cure epoxy adhesive system developed for structural bonding applications on vertical or overhead surfaces where its instant develop..
|
|||
| Glass Transition Temp, Tg | 45.0 °C | 113 °F | TM R050-25 |
|
Resinlab® EP1190 Flame Retardant Epoxy Casting Resin
Resinlab™ EP1190 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Proje..
|
|||