Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = 50.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 50.0 °C
122 °F
ISO 11357-1
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
Glass Transition Temp, Tg 50.0 °C
122 °F
ISO 11357-1
Murtfeldt Murlubric® Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
Glass Transition Temp, Tg 50.0 °C
122 °F
ISO 11357-1
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..
Glass Transition Temp, Tg 50.0 °C
122 °F
ISO 11357-1
Murtfeldt Murylon® B Nylon 6
Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope..
Glass Transition Temp, Tg 50.0 °C
122 °F
Permabond ET505 Epoxy Resin
PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas..
Glass Transition Temp, Tg 50.0 °C
122 °F
Lucite International Elvacite ® 2697 Acrylic Resin
Elvacite® 2697 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. Elvacite® 2697 is useful in clear, translucent or pigmented metal lacquers. It is a fast dissolvi..
Glass Transition Temp, Tg 50.0 °C
122 °F
ASTM E1356
SK Chemicals SKYTHANE® US210 Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Glass Transition Temp, Tg 50.0 °C
122 °F
Ultimate Tg; TMA
Tra-Con Tra-Bond 516H02 Fiber Optic Adhesive
TRA-BOND 516H02 is a low viscosity, room temperature or low temperature curing fiber optic adhesive with good stress relief, high adhesion, and low shrinkage upon cure. TRA-BOND 516H02 contains very..
Glass Transition Temp, Tg 50.0 °C
122 °F
Ultimate Tg; TMA
Tra-Con Tra-Bond 546S02 Low Viscosity UV Curable Adhesive
TRA-BOND 546S02 is a low viscosity UV curable adhesive exhibiting exceptional adhesion to glass. TRA-BOND 546S02 is designed to be semi-flexible resulting in stress free bonds to glass and other sub..
Glass Transition Temp, Tg 50.0 °C
122 °F
Ultimate Tg
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive
TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an..
Glass Transition Temp, Tg 50.0 °C
122 °F
Ultimate Tg
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive
TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste s..
Glass Transition Temp, Tg 50.0 °C
122 °F
Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
Glass Transition Temp, Tg 50.0 °C
122 °F
ETM 300-90
ExxonMobil ESCOREZ™ 1102 (Americas) Petroleum Hydrocarbon Resin
Aliphatic hydrocarbon resin which is designed for use in a varity of applicaitons.Availability: Central America, North America and South AmericaInformation provided by ExxonMobil Chemical
Glass Transition Temp, Tg >= 50.0 °C
>= 122 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy
Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..
Glass Transition Temp, Tg >= 50.0 °C
>= 122 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy
Material Description: A two component, black colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..
Glass Transition Temp, Tg >= 50.0 °C
>= 122 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® 730 Unfilled Black General and Structural Grade Epoxy
Material Description: A two component, room temperature curing, general and structural grade epoxy. It can be used for adhesive, sealing, and encapsulating applications in medical, xray device, fil..
Glass Transition Temp, Tg >= 50.0 °C
>= 122 °F
Epoxy Technology EPO-TEK® B9021-1 Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
Glass Transition Temp, Tg >= 50.0 °C
>= 122 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy
Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology
Glass Transition Temp, Tg 50.0 °C
122 °F
dry, dynamic; DIN 53 736
Hippe PA 66 Nylon 66
The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec..
Glass Transition Temp, Tg 50.0 °C
122 °F
DAM; 10°C/min; ISO 11357-1/-2
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers
Glass Transition Temp, Tg 50.0 °C
122 °F
TM R050-25
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin
Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate ..
Glass Transition Temp, Tg 50.0 °C
122 °F
TM R050-25
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive
Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili..
Glass Transition Temp, Tg 50.0 °C
122 °F
TM R050-25
Resinlab® EP1305LV Black Epoxy Casting Resin
Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..
Copyright © lookpolymers.com All Rights Reserved