| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | DMA, E" |
|
Proto3000 Accura® 50 Plastic Stereolithography (SLA) Prototyping Polymer
Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey..
|
|||
| Glass Transition Temp, Tg | 62.0 - 65.0 °C | 144 - 149 °F | DMA, E |
|
Proto3000 Objet RGD525 High Temperature Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | DSC, both heating and cooling speeds of 20°C/min |
|
Noltex Soarnol® D2908 Ethylene Vinyl Alcohol Copolymer
Ethylene content 29 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | DSC, both heating and cooling speeds of 20°C/min |
|
Noltex Soarnol® DT2903 Ethylene Vinyl Alcohol Copolymer
Very low ethylene content, high gas barrier for packaging dry products or for use in packaging material used at normal temperature and humidity. Ethylene content 29 mol%. Volatile matter 0.3%.The ..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | Dynamic Viscoelasticity |
|
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | Dynamic Viscoelasticity |
|
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | DMA, E" |
|
Huntsman RenShape® SL 7820 Stereolithography Plastic
RenShape® SL 7820 stereolithography material is a white, low viscosity and stable liquid that produces strong black models and prototypes with good surface fi nish and detail, and ABS-like appear..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | |
|
SpinTech Veritexâ„¢ Shape Memory Polymer Composite
Veritexâ„¢ is a fiber-reinforced composite that uses a shape memory polymer, VeriflexÂ, as the matrix. This allows Veritex to easily change shape above its activation temperature. At lower tempe..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | Ultimate Tg |
|
Tra-Con Tra-Cast 3104 Low Viscosity Epoxy Casting Compound
TRA-CAST 3104 is a low viscosity, room temperature cure epoxy casting system developed for high performance production encapsulation and impregnating applications where filling fine intricate free s..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | Ultimate Tg |
|
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System
TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | Ultimate Tg |
|
Tra-Con Tra-Duct 29121 Snap Cure Conductive Silver Epoxy Adhesive
TRA-DUCT 29121 is 100% solids, two component silver filled epoxy designed for chip bonding in microelectronic and optoelectronic applications. TRA-DUCT 29121 is a soft, smooth paste. This two-part f..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | Ultimate Tg |
|
Tra-Con Tra-Duct 921H01
Information provided by Tra-Con Inc.
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | Ultimate Tg |
|
Tra-Con Tra-Bond 2101 General Purpose Epoxy Adhesive
TRA-BOND 2101 is a medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of its superior structural, mechanical and ele..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | DMA, E" |
|
3D Systems Accura® 50 Plastic for SLA® Systems
Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.ApplicationsFunctional components for assemblies, mock-ups and te..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | |
|
Armstrong A-12-T Epoxy Adhesive
Provides the same basic properties as A-12, but in thixotropic, non-sag, easily-brushable paste form. An ideal material for use where adhesive flow during cure cannot be tolerated. A-12-T meets t..
|
|||
| Glass Transition Temp, Tg | 62.0 - 65.6 °C | 144 - 150 °F | DMA, E" |
|
3D Systems Accura® 40 Plastic for SLA® Systems
40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | DMA, E" |
|
3D Systems Accura® 10 Plastic for SLA® Systems
Accura 10 "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsGeneral use prototyping for many uses, including:Enclosures, covers and casesCellular/mobile ph..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | TM R050-25 |
|
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive
EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go..
|
|||
| Glass Transition Temp, Tg | 62.0 °C | 144 °F | |
|
Atom Adhesives AA-BOND 2101 Epoxy Adhesive
AA-BOND 2101 is a clear medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of superior structural, mechanical and el..
|
|||