Polymer Property : CTE, linear, Transverse to Flow = 20.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 37.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
20.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp DF008P PC
LNP THERMOCOMP* DF008P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the ..
CTE, linear, Transverse to Flow 37.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
20.6 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON RE007 PA 66
LNP* STAT-KON* RE007 is a compound based on PA66 resin containing 35% Carbon Fiber. Added features include: Electrically Conductive.
CTE, linear, Transverse to Flow 37.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
20.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp DF008P PC (Asia Pacific)
LNP* THERMOCOMP* DF008P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the..
CTE, linear, Transverse to Flow 37.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
20.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ASTM E 228
DuPont Performance Polymers VESPEL TP-8549 Polyimide
Thermoplastic parts from filled PI (polyimide) for high mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Performance..
CTE, linear, Transverse to Flow 37.0 µm/m-°C
20.6 µin/in-°F
z direction
Arlon AR1000 Glass, PTFE and Micro-Dispersed Ceramic
Used in the RF and microwave industries.Information provided by Arlon Materials for Electronics (MED).
CTE, linear, Transverse to Flow 37.0 - 80.0 µm/m-°C
20.6 - 44.4 µin/in-°F
Average value: 50.4 µm/m-°C Grade Count:5
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..