| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
40.1
µm/m-°C @Temperature -30.0 - 30.0 °C |
22.3
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E 831 |
|
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6
LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity.
|
|||
| CTE, linear, Transverse to Flow |
40.1
µm/m-°C @Temperature -30.0 - 30.0 °C |
22.3
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E 831 |
|
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6
4.0 specific gravity, Nylon 6
|
|||