Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 45.0 µm/m-°C
25.0 µin/in-°F
Average below Tg, Result based on 450GL30; ISO 11359
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
CTE, linear, Transverse to Flow 45.0 - 70.0 µm/m-°C
25.0 - 38.9 µin/in-°F
Average value: 59.8 µm/m-°C Grade Count:7
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 20.0 °C
25.0 µin/in-°F
<br>@Temperature 68.0 °F
Cookson Group Plaskon® S-7LA Molding Compound &nbsp;(discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 20.0 °C
25.0 µin/in-°F
<br>@Temperature 68.0 °F
Cookson Group Plaskon® S-7P Epoxy Encapsulant &nbsp;(discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically ..
CTE, linear, Transverse to Flow 45.0 - 68.0 µm/m-°C
25.0 - 37.8 µin/in-°F
Average value: 54.5 µm/m-°C Grade Count:4
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
25.0 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ G1352A-M41 Nylon, 35% Glass Filled
Low friction reinforced injection grade.Main Features:Low friction coefficientAbrasion resistanceExamples of applications:Friction and wear applicationGear and wheel
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
25.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA
LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
25.0 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
25.0 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
25.0 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem 2410F PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). UL94 V0 and 5VA listing. US FDA and European Food contact approved. Effective June, 2007 this grade will no longer be supported with b..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
25.0 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
25.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI
LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
25.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp JF003L PES
LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
25.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK
LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
25.0 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear
LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
25.0 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East)
LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON MV006S PP
LNP* VERTON* MV006S is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Structural.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON MV006SU PP (Asia Pacific)
LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
25.0 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East)
NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306.
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 20.0 °C
25.0 µin/in-°F
<br>@Temperature 68.0 °F
TMA
Vyncolit X6151 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump ..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 20.0 °C
25.0 µin/in-°F
<br>@Temperature 68.0 °F
TMA
Vyncolit X640 Resole Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 20.0 °C
25.0 µin/in-°F
<br>@Temperature 68.0 °F
TMA
Vyncolit X680 Novolac Phenolic
Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with t..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 20.0 °C
25.0 µin/in-°F
<br>@Temperature 68.0 °F
TMA
Vyncolit X689 Novolac Phenolic
Glass fiber filled and molybdeendisulfide modified phenolic molding compound with excellent mechanical and thermal properties and lower thermal expansion coefficient. It has excellent friction prop..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
25.0 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® 46SF5030 PA46-GF30 FR(17)
30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow
CTE, linear, Transverse to Flow 45.0 µm/m-°C
25.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
25.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
25.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45
Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
25.0 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 45.0 - 80.0 µm/m-°C
25.0 - 44.4 µin/in-°F
Average value: 65.5 µm/m-°C Grade Count:10
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
CTE, linear, Transverse to Flow 45.0 µm/m-°C
25.0 µin/in-°F
TMA
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound
BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri..