| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
38.9
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Cycoloy® EFX830ME PC
Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering metallic / sparkle look with minimal flow line visibilityThis data was supplied by SABIC-..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
38.9
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East)
LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
38.9
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EXL6013 PC (Europe-Africa-Middle East)
LEXAN EXL6013 is especially developed for applications requiring a high impact performance combined with an improved chemical resistance over standard polycarbonate.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
38.9
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® EX2078X PC (Europe-Africa-Middle East)
Lexan* EX2078X polycarbonate resin, MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retardant, halogen free per DIN VDE 0472 Part 815, mold release, UV stabilized, translu..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Apec® 1700 Polycarbonate
(discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade
(discontinued **)
Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially sui..
|
|||
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Pocan® BF 8230 000000 PBT, 30% Glass Fiber
PBT, 30% glass spheres/glass fibers, injection molding, flame retardant, low tendency to warp, improved surface finish
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359 |
|
Teijin Panlite® LN-3000RM High Light Reflection, Halogen-Free Flame Resistant Polycarbonate Resin
Polycarbonate-resin-based halogen-free flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even a..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359 |
|
Teijin Panlite® LS-2250 Friction and Abrasion Resistant Polycarbonate Resin
It is compounded with fluorine powder to improve friction and abrasion resistance, meeting UL 94 V-2. The friction and abrasion resistance is superior than that of polyamidoacetal, maintaining excel..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
38.9
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Noryl GTX VP7133 PPE+PA (Europe-Africa-Middle East)
Noryl GTX VP7133 is an unfilled extrusion grade which offers high heat resistance in combination with high meltstrength.The material is especially designed for thermal break profiles which are used ..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
38.9
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Noryl HB1525 PPE+HIPS (Europe-Africa-Middle East)
NORYL HB1525 is a 15 % short glass fibre reinforced material with a HDT/A of 115°C according ISO 75. NORYL HB1525 is an easy flow material designed for applications where dimensional stability an..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
38.9
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL PX5511E PPE+HIPS (Europe-Africa-Middle East)
Noryl PX5511E is an unfilled material with good flow and chemical resistance against cleaners. Noryl PX5511E is developed for personal care appplications.
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359 |
|
Teijin Panlite® LV-2225Z Transparent and Weather Resistant grade Polycarbonate Resin
Injection molding grade that is necessary to be slightly high fluidity. It has weather resistance, mold release property and is bluish-tinted to exhibit clear color.Applications:Components of electr..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
38.9
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN1 is a standard 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1 can be used for all applications where a higher modulus is required. NORYL GFN1 is ava..
|
|||
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
|
Covestro Apec® 1695 Polycarbonate
Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Apec® HT KU 1-9371 High-Heat Polycarbonate
Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated ..
|
|||
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | dry; ISO 11359-1/-2 |
|
DSM Akulon® K224-G6-FC 99.99.99 PA6-GF30
30% Glass Reinforced, Food Contact Grade
|
|||
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | dry; ISO 11359-1/-2 |
|
DSM Akulon® K224-LG6 /E PA6-GF30
30% Glass Reinforced, Injection Molding, Improved UV-stability
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Akulon® S223-HG6 (Dry) 30% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Makrolon® 2207 Polycarbonate, Injection Grade
Exceptionally good flow injection molding grade with easy mold release and UV stabilizer, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Akulon® Ultraflow™ K-FG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Makrolon® 3208 Polycarbonate
Injection molding and extrusion grade with high viscosity, BgVV- and FDA grade for food contact applications, yields especially tough parts, better resistance to hot water.Information provided by Ba..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Makrolon® 6465 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding with easy mold burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offici..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Makrolon® KU 1-1243 Polycarbonate, UV-Stabilized
Pseudoplastic behavior and high viscosity extrusion grade with UV stabilizer and easy mold release, special grade for twin-wall sheet.Information provided by Bayer.As of 1 September 2015, Bayer Mate..
|
|||
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | dry; ISO 11359-1/-2 |
|
DSM Novamid® 1010GN2-20 NAT/BK37 PA6-GF20 FR(17)
20% Glass Reinforced, Flame Retardant
|
|||
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | dry; ISO 11359-1/-2 |
|
DSM Novamid® 1013G30 1 NA PA6-GF30
30% Glass Reinforced, Injection Molding
|
|||
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30
Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: ..
|
|||
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
|
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade
Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Arkema Group Orgalloy® RS 6015 BV Nylon 6 Alloy, Glass Fiber + Bead Filled (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties..
|
|||
| CTE, linear, Transverse to Flow |
70.0
µm/m-°C <br>@Temperature 20.0 °C
|
38.9
µin/in-°F <br>@Temperature 68.0 °F
|
ISO data |
|
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||