| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
22.2
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 3441R PC (Europe-Africa-Middle East)
Lexan 3441R is a medium viscosity, 10% glass reinforced polycarbonate grade, compliant with European food contact regulation EC Directive 2002/72/EC. The grade is especially designed for application..
|
|||
| CTE, linear, Transverse to Flow | 40.0 - 80.0 µm/m-°C | 22.2 - 44.4 µin/in-°F | Average value: 58.0 µm/m-°C Grade Count:5 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
22.2
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East)
CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C <br>@Temperature 20.0 °C
|
22.2
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Akulon® K-FHG12 (Dry) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C <br>@Temperature 20.0 °C
|
22.2
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| CTE, linear, Transverse to Flow | 40.0 - 102 µm/m-°C | 22.2 - 56.7 µin/in-°F | Average value: 61.4 µm/m-°C Grade Count:16 |
|
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
|
|||
| CTE, linear, Transverse to Flow | 40.0 - 87.0 µm/m-°C | 22.2 - 48.3 µin/in-°F | Average value: 51.8 µm/m-°C Grade Count:4 |
|
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
|
|||
| CTE, linear, Transverse to Flow | 40.0 - 55.0 µm/m-°C | 22.2 - 30.6 µin/in-°F | Average value: 44.3 µm/m-°C Grade Count:7 |
|
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
|
|||
| CTE, linear, Transverse to Flow |
40.0
-
50.0
µm/m-°C <br>@Temperature 20.0 °C
|
22.2
-
27.8
µin/in-°F <br>@Temperature 68.0 °F
|
TMA |
|
Vyncolit X681 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica..
|
|||
| CTE, linear, Transverse to Flow |
40.0
-
50.0
µm/m-°C <br>@Temperature 20.0 °C
|
22.2
-
27.8
µin/in-°F <br>@Temperature 68.0 °F
|
TMA |
|
Vyncolit 2530 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba..
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | TMA |
|
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic
Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by ..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C <br>@Temperature 20.0 °C
|
22.2
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Baygal® 90 IK 51 Polyurethane
Uses: Suitable for the solid insulation of measuring transducers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its ne..
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
|
DSM Arnite® AV2 370 XL-T PET-GF35
35% Glass Reinforced, Low Outgassing, Thermal conductive material
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | dry; ISO 11359-1/-2 |
|
DSM Stanyl® OCD2300 BLK PA46-GF50
50% Glass Reinforced, Heat Stabilized
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60
Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p..
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60
Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll..
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60
Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following ..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C <br>@Temperature 20.0 °C
|
22.2
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| CTE, linear, Transverse to Flow |
40.0
µm/m-°C <br>@Temperature 20.0 °C
|
22.2
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Makroblend® UT-640 G Polycarbonate + Polyester Blend
Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe..
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
|
DSM Arnite® AV2 370 XL PET-GF35
35% Glass Reinforced, Low Outgassing
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60
Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac..
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50
Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl..
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
|
Barlog Plastics KEBATER BF250 PBT, 50% glass fiber reinforced, food grade
PBT-GF50Information provided by BARLOG plastics GmbH.
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM E 831 |
|
Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style ..
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | z direction |
|
Arlon AD430 Glass, PTFE and Micro-Dispersed Ceramic
High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED).
|
|||
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | TMA |
|
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound
Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C)...
|
|||
| CTE, linear, Transverse to Flow | 40.0 - 85.0 µm/m-°C | 22.2 - 47.2 µin/in-°F | Average value: 61.8 µm/m-°C Grade Count:10 |
|
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
|
|||