Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 20.0 °C
43.3 µin/in-°F
<br>@Temperature 68.0 °F
ISO data
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry) &nbsp;(discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 20.0 °C
43.3 µin/in-°F
<br>@Temperature 68.0 °F
Eastman Eastalloy DA105 PC+PET Copolyester/Polycarbonate &nbsp;(discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 20.0 °C
43.3 µin/in-°F
<br>@Temperature 68.0 °F
Cookson Group Plaskon® 440S Mineral Filled Novolac Epoxy Molding Compound &nbsp;(discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.Combines exceptional reliability with wide process latitude. This material is designed to encapsulate a wide range of semiconduc..
CTE, linear, Transverse to Flow 78.0 - 130 µm/m-°C
43.3 - 72.2 µin/in-°F
Average value: 103 µm/m-°C Grade Count:3
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 20.0 °C
43.3 µin/in-°F
<br>@Temperature 68.0 °F
ISO data
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry) &nbsp;(discontinued **)
Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av..
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
43.3 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp DP003XXP PC (Europe-Africa-Middle East)
LNP* LUBRICOMP* DP003XXP is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa..
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS
LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant.
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
43.3 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL369 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFL369 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame Retardant, internally lubricated
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS
LNP* LUBRICOMP* ZP001XXP is a compound based on PPE+PS resin containing 5% PTFE/Silicone. Added features of this material include: Wear Resistant.
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP DX09402 PC
LNP* THERMOCOMP* DX09402 is a compound based on Polycarbonate containing Proprietary Filler(s).
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
43.3 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66
LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare.
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 20.0 °C
43.3 µin/in-°F
<br>@Temperature 68.0 °F
Eastman Eastapak 9921 PET
ISO data as provided by the manufacturer, Eastman Chemical
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 20.0 °C
43.3 µin/in-°F
<br>@Temperature 68.0 °F
Eastman Eastar DN004 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
CTE, linear, Transverse to Flow 78.0 µm/m-°C
43.3 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® RE19051 BK507 Polyethylene Terephthalate (PET)
40% Glass/Mineral Reinforced Flame Retardant Polyethylene Terephthalate Rynite RE19051 BK507 is a 40% glass and mineral reinforced flame retardant polyethylene terephthalate black resin.Information ..
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
43.3 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide AG6ST01 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding
Staramide AG6ST01 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
43.3 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
43.3 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded
Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 78.0 µm/m-°C
43.3 µin/in-°F
ISO 11359
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..
CTE, linear, Transverse to Flow 78.0 - 190 µm/m-°C
43.3 - 106 µin/in-°F
Average value: 108 µm/m-°C Grade Count:6
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 20.0 °C
43.3 µin/in-°F
<br>@Temperature 68.0 °F
ISO data
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry) &nbsp;(discontinued **)
Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
CTE, linear, Transverse to Flow 78.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
43.3 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON RC008 PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* RC008 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.