Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® GPM5500 ABS (Europe-Africa-Middle East)
CYCOLAC GPM5500 is a multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500 has a wide processing window. It is recommended for application..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East)
CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® C3100 PC+ABS (Europe-Africa-Middle East)
C3100 is blow moulding/extrusion grade offering low temperature ductility, high heat resistance and high meltstrength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East)
XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
CTE, linear, Transverse to Flow 80.0 - 110 µm/m-°C
44.4 - 61.1 µin/in-°F
Average value: 89.3 µm/m-°C Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® B 40 FAM 000000 Nylon 6, Film Grade
PA 6 film grade of high viscosity with high slip agent and lubricant content, not nucleatedApplication Examples: flat and blown film with good surface slip and smoothness - including in the freshly ..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6, 40% Glass Fiber + Mineral
PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® B 4235 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PA (Europe-Africa-Middle East)
NORYL GTX830 a 30% glass reinforced grade which offers an excellent combination of chemical/heat resistance in combination with stiffness.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East)
Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duranex® 6370B Polybutylene Terephthalate (PBT), Anisotropy improvement, 30% GB filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradegeneral purposecompared to FR 3000 improved chemical resistance and stress cracking behaviorVicat/B 120 temperature = 97 °CUL 94 V-0 at 1.5 mmPreprocessingMax. Water content
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
Covestro Bayblend® FR 3001 Polycarbonate + ABS Blend
Key Features:Flame retarding agentUnfilledFlame retardantSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separat..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled
Injection molding grade20 % glass fiber filledtensile modulus = 5900 MPaVicat/B 120 temperature = 134 °CPreprocessingMax. Water content
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
Covestro Baydur® 40 Polyurethane
Rigid integral skin polyurethane foam for lightweight moldings. Sandwich structure gives a high stiffness-to-weight ratio.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience ..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® 46HF5041LW (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow, Low Warpage (North America)
Information provided by DSM Engineering Plastics.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30
Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 4028 nat PA12/MACMI
Product description: Grilamid XE 4028 natural is a transparent thermoplastic polyamides based on aliphatic, cycloaliphatic and aromatic blocks. Grilamid XE 4028 natural offers a variety of interesti..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding
Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide A40 PA66, Extrusion
Staramide A40 is Unreinforced, High Viscosity Polyamide 66, Extrusion ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide B28H PA6, Heat Stabilized, Injection Molded
Staramide B28H is a Heat Stabilized, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TRV-4X9 PAMACM12-GF40
Product description: Grilamid TRV-4X9 is an amorphous, cycloaliphatic polyamide with 40% glass fibre reinforcement. Grilamid TRV-4X9 characterises itself through the following features: Very low shr..
CTE, linear, Transverse to Flow 80.0 - 120 µm/m-°C
<br>@Temperature 23.0 - 55.0 °C
44.4 - 66.7 µin/in-°F
<br>@Temperature 73.4 - 131 °F
ISO 11359-1/-2
BASF Ultramid® Seal-Fit PA6/66 (Dry)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TRVX-50X9 nat PAMACM12-GF50
Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and..
Copyright © lookpolymers.com All Rights Reserved