Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 50.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1,-2
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers
PA 66, 15% glass fibers, injection molding, heat-ageing stabilized
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, improved notched impact strength and energy absorption under biaxial impact load, good heat-ageing resistance
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral
PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS.
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® B 3235 901510 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS.
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Noryl PX9406N PPE+HIPS (Europe-Africa-Middle East)
Noryl PX9406N is an unfilled, halogen free (according VDE/DIN 472 part 813) flame retardant material with medium heat resistance. This material is V0 at 1.0 mm according to UL94.This data was suppli..
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RA004 is a compound based on Nylon 66 resin containing Aramid Fiber.
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX976 PPE+PA (Europe-Africa-Middle East)
NORYL GTX976 is a material especially designed for electrostatic painting and powder coating applications. This material combines high impact performance with conductivity in an unique way.This data..
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL HF185 PPE+HIPS (Europe-Africa-Middle East)
NORYL HF185 is an unfilled, halogen free (according VDE/DIN 472 part 815), flame retardant and easy flow NORYL grade.
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PX1185 PPE+HIPS (Europe-Africa-Middle East)
NORYL PX1185 is a special NORYL grade developed for extrusion of automotive trims. NORYL PX1185 offers high heat resistance and good impact performance.
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duranex® 3300 Polybutylene Terephthalate (PBT), Standard, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duranex® 3306 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® 2S 20 nat PA610
Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product..
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® GM-4H PA*-MD40
Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G..
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50
Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TR 55 LX PA12/MACMI
Product description: Grilamid TR 55 LX natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 LX natural offers outstanding prop..
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TSS/4 LF 1 PA666
Product description: Grilon TSS/4 LF 1 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 1% lubricant (molybdenum disulphide). Grilon TSS/4 LF 1 has the following import..
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Minlon® 10B140 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66Minlon 10B140 NC010 is a 40% mineral reinforced polyamide 66 for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TR 90 LS PAMACM12
Product description: Grilamid TR 90 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LS natural contains a processing a..
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TR 90 UV PAMACM12
Product description: Grilamid TR 90 UV natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid 90 UV natural offers outstanding propert..
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
50.0 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Barlog Plastics KEBATER BF115 PBT, 15% glass fiber reinforced
PBT-GF15Information provided by BARLOG plastics GmbH.
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT6007* offers an exceptional low-temperature impact strength, good flowability and..
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® DP 2801 000000 Nylon 66
PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free
Copyright © lookpolymers.com All Rights Reserved