Polymer Property : CTE, linear, Transverse to Flow = 66.7 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 20.0 °C
66.7 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® S223-P2 Impact Modified Nylon 66 (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66  (Unverified Data**)
Zytel® ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance, high productivity and laser markability.Information provided by DuPont
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding, flame retardant
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® DP 2004 000000 PBT
PBT, non-reinforced, injection molding, halogen free flame retardant
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® B 1505 000000 PBT
PBT, non-reinforced, injection molding, extrusion
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 80.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East)
VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009. 30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 60.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP (Europe-Africa-Middle East)
LNP* Thermocomp* MB006S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 80.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East)
VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin.
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature -40.0 - 40.0 °C
66.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East)
Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duranex® 3105A Polybutylene Terephthalate (PBT), Epoxy adhesion improved, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I
Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro..
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® EBV-2H PA6-GF20
Product description: Grilon EBV-2H is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 20% glass fibers. Grilon EBV-2H has the following important properties: High melt streng..
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® LKN-5H PA12-GB50
Product description: Grilamid LKN-5H is a 50% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g..
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 100ST BK602 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST BK602 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 60.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded
AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 60.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded
Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar.
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Barlog Plastics KEBAFORM C 520.0 POM Copolymer unreinforced
POMInformation provided by BARLOG plastics GmbH.
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® M25-44/M25S Acetal Co-polymer (POM), Standard, High viscosity
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® M90-48 Acetal Co-polymer (POM), Antistatic, General
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® M90-71 Acetal Co-polymer (POM), Heat resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature 23.0 - 80.0 °C
66.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East)
VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® BGZ-15/2 PA6-GF15
Product description: Grilon BGZ-15/2 is a heat stabilized and impact modified PA6 injection molding grade with 15% glass fibers. Grilon BGZ-15/2 has the following important properties: Good impact s..
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® BZ 1 PA6
Information provided by EMS Grivory