Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 80.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 40.0 - 80.0 µm/m-°C
22.2 - 44.4 µin/in-°F
Average value: 58.0 µm/m-°C Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
CTE, linear, Transverse to Flow 17.0 - 80.0 µm/m-°C
9.44 - 44.4 µin/in-°F
Average value: 55.4 µm/m-°C Grade Count:12
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
CTE, linear, Transverse to Flow 26.4 - 80.0 µm/m-°C
14.7 - 44.4 µin/in-°F
Average value: 58.5 µm/m-°C Grade Count:7
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma..
CTE, linear, Transverse to Flow 70.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry)
Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade.
CTE, linear, Transverse to Flow 70.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry)
Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi..
CTE, linear, Transverse to Flow 70.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
CTE, linear, Transverse to Flow 70.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
CTE, linear, Transverse to Flow 70.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
CTE, linear, Transverse to Flow 45.0 - 80.0 µm/m-°C
25.0 - 44.4 µin/in-°F
Average value: 65.5 µm/m-°C Grade Count:10
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
CTE, linear, Transverse to Flow 10.0 - 80.0 µm/m-°C
5.56 - 44.4 µin/in-°F
Average value: 33.3 µm/m-°C Grade Count:3
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
CTE, linear, Transverse to Flow 40.0 - 80.0 µm/m-°C
22.2 - 44.4 µin/in-°F
Average value: 59.3 µm/m-°C Grade Count:21
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..
CTE, linear, Transverse to Flow 45.0 - 80.0 µm/m-°C
25.0 - 44.4 µin/in-°F
Average value: 62.8 µm/m-°C Grade Count:18
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
CTE, linear, Transverse to Flow 37.0 - 80.0 µm/m-°C
20.6 - 44.4 µin/in-°F
Average value: 50.4 µm/m-°C Grade Count:5
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..