| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Transverse to Flow |
150
µm/m-°C <br>@Temperature 23.0 - 55.0 °C
|
83.3
µin/in-°F <br>@Temperature 73.4 - 131 °F
|
ISO 11359-1,-2 |
|
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6
PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
|
|||
| CTE, linear, Transverse to Flow |
150
µm/m-°C <br>@Temperature 23.0 - 55.0 °C
|
83.3
µin/in-°F <br>@Temperature 73.4 - 131 °F
|
ISO 11359-1, -2 |
|
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified
PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS.
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning ..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Durethan® BKV 215 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning ..
|
|||
| CTE, linear, Transverse to Flow |
150
µm/m-°C <br>@Temperature 23.0 - 55.0 °C
|
83.3
µin/in-°F <br>@Temperature 73.4 - 131 °F
|
ISO 11359-1, -2 |
|
Lanxess Durethan® TP 142-011 900116 Nylon 6
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| CTE, linear, Transverse to Flow |
150
µm/m-°C <br>@Temperature -30.0 - 100 °C
|
83.3
µin/in-°F <br>@Temperature -22.0 - 212 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 9712 PP
SABIC® PPcompound 9712 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st..
|
|||
| CTE, linear, Transverse to Flow |
150
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
83.3
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics LNP THERMOCOMP HF006EU PA11 (Europe-Africa-Middle East)
LNP* THERMOCOMP* HF006EU is a compound based on PA 11 resin containing Glass Fiber. Added features include: Easy Molding, UV-Stabilized.
|
|||
| CTE, linear, Transverse to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Transverse to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® EM630-H Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Transverse to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® PL380 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Transverse to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® PL381 Injection Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
DSM Arnitel® PL381-H TPC-ET
Injection Molding
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® 2S 25 W 20 HL X black 9992 PA610
Product Description: Grilamid 2S 25 W 20 HL X black 9992 is a semi-flexible high viscosity heat stabilized, impact modified and plasticized Polyamide 610, especially suitable for extrusion applicati..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I
Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® BFZ 3 PA6
Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® BG-25 HM PA6-GF25
Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® BRZ 247 W PA6
Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® BZ 3 PA6
Information provided by EMS Grivory
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® L 25 NZ ESD PA12
Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of ..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® LV-23 ESD PA12-GF23
Product description: Grilamid LV-23 ESD is a 20% fiber reinforced, anti-static injection molding grade Polyamide 12 (PA12). Grilamid LV-23 ESD is heat stabilized, is easy to process and demold. The ..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® LV-2A NZ PA12-GF20
Product description: Grilamid LV-2A NZ is a high viscosity polyamide 12 with 20% glass fibers and improved hydrolysis resistance compared to standard polyamide 12 materials. Grilamid LV-2A NZ has a ..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® LV-2H PA12-GF20
Product description: Grilamid LV-2H is a 20% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30
Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30
Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® LV-3H PA12-GF30
Product description: Grilamid LV-3H is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® TSZ 1 PA666
Product description: Grilon TSZ 1 is a heat stabilized, normal viscosity, impact modified PA66 + PA6 injection molding grade. Grilon TSZ 1 has the following important properties: Excellent flow beha..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® TSZ 3 PA666
Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® XE 4128 black 9221 PA610
Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | z, above Tg; IPC TM-650 2.4.24 |
|
Arlon 84N Polyimide Laminate and Prepreg
84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay..
|
|||
| CTE, linear, Transverse to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® LC-15H black PA12-CF15
Product description: Grilamid LC-15H black is a Polyamide 12 injection molding product reinforced with 15% carbon fibers. The product is inherently black and is only available in this color.Main Att..
|
|||