| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear |
160
µm/m-°C <br>@Temperature 90.0 - 150 °C
|
88.9
µin/in-°F <br>@Temperature 194 - 302 °F
|
T>Tg; ASTM E831-93 |
|
Proto3000 Accura® 45HC Plastic Stereolithography (SLA) Prototyping Polymer
A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.Benefits:Fast build speed:Provides build speeds that are sign..
|
|||
| CTE, linear |
160
µm/m-°C <br>@Temperature 200 - 300 °C
|
89.0
µin/in-°F <br>@Temperature 392 - 572 °F
|
ASTM E831 |
|
3M Dyneon™ CC503 PTFE, 15% Mineral Filled
(discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings - FDA compliant, valve seats, seals.Data provided by Dyneon.
|
|||
| CTE, linear |
160
µm/m-°C <br>@Temperature 20.0 - 100 °C
|
88.9
µin/in-°F <br>@Temperature 68.0 - 212 °F
|
DIN 52328 |
|
Fluorseals PTFE Unfilled
Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
|
|||
| CTE, linear |
160
µm/m-°C <br>@Temperature <=150 °C
|
88.9
µin/in-°F <br>@Temperature <=302 °F
|
ISO E 831 |
|
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy
Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato..
|
|||
| CTE, linear |
160
µm/m-°C <br>@Temperature 20.0 °C
|
88.9
µin/in-°F <br>@Temperature 68.0 °F
|
Alpha 2 |
|
Tra-Con Tra-Bond 226U01 High Temperature Controlled Flow Adhesive
TRA-BOND 226U01 is a one-part, controlled flow adhesive with high temperature resistance.Information provided by Tra-Con Inc.
|
|||
| CTE, linear |
160
µm/m-°C <br>@Temperature 90.0 - 150 °C
|
88.9
µin/in-°F <br>@Temperature 194 - 302 °F
|
T>Tg; ASTM E831-93 |
|
3D Systems Accura® 45HC Plastic for SLA® Systems
A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.ApplicationsHigh temperature testing:Automotive "under-the-ho..
|
|||