| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 43.0 °C | 104 - 109 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_8425 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 43.0 °C | 104 - 109 °F | ASTM D648-06 |
|
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
|
|||