Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 136 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
SABIC Innovative Plastics Lexan® 243R PC (Europe-Africa-Middle East)
LEXAN 243R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved.
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
SABIC Innovative Plastics Lexan® 940A PC (Europe-Africa-Middle East)
LEXAN 940A is a medium viscosity flame retardant grade, especially suitable for electrical applications.
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
SABIC Innovative Plastics Lexan® 945AU PC (Europe-Africa-Middle East)
Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East)
Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Faradex DS0036IP PC
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
SABIC Innovative Plastics Lexan® 144R PC (Europe-Africa-Middle East)
Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
SABIC Innovative Plastics Lexan® HP4 PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold ..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics PC1500 PC
PC1500 resin is a medium-high flow (MFR = 15 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC
LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C

@Thickness 6.40 mm
277 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced
High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung ..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1,-2
Covestro Makrolon® 1954 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Low viscosity• UV st..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1,-2
Covestro Makrolon® 2407 MAS056 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1/-2
Covestro Makrolon® 2558 Polycarbonate
ISO 7391-PC,MR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for ETO and steam sterilization at 121 °CComplies with the requirements of FDA-modified ISO 10993-1 and USP Class..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1,-2
Covestro Makrolon® 2607 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1,-2
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1/-2
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Covestro Makrolon® 2807 Polycarbonate, Injection Grade
Medium flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1/-2
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1,-2
Covestro Makrolon® 6165 X Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Low..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Covestro Makrolon® 6465 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding with easy mold burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offici..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1/-2
Covestro Makrolon® AL2447 Polycarbonate
ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa..
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
ISO 75-1,-2
Covestro Makrolon® FU1007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
Deflection Temperature at 0.46 MPa (66 psi) 136 - 149 °C
277 - 300 °F
Average value: 145 °C Grade Count:46
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
Deflection Temperature at 0.46 MPa (66 psi) 136 - 145 °C
277 - 293 °F
Average value: 140 °C Grade Count:5
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
Copyright © lookpolymers.com All Rights Reserved