| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 65.0 - 72.8 °C | 149 - 163 °F | Average value: 68.7 °C Grade Count:5 |
|
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 70.0 - 73.0 °C | 158 - 163 °F | Average value: 72.0 °C Grade Count:3 |
|
Overview of materials for High Density Polyethylene (HDPE), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 58.0 - 73.0 °C | 136 - 163 °F | Average value: 68.0 °C Grade Count:3 |
|
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 40.0 - 72.8 °C | 104 - 163 °F | Average value: 44.7 °C Grade Count:18 |
|
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..
|
|||