Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 194 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 - 90.0 °C
180 - 194 °F
after thermal post treatment procedure A; ASTM D648-06
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer
Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to..
Deflection Temperature at 0.46 MPa (66 psi) 88.0 - 90.0 °C
190 - 194 °F
C.O.I.M. EXTER S® S 501 Neopentylic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 501: Resin for high-..
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 90.0 °C
185 - 194 °F
Average value: 87.6 °C Grade Count:4
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim..